Understanding Heavy and Light Hole Transport Dynamics in Diamond Through Monte Carlo Simulations and Experiments
Paper details
Section titled “Paper details”| Field | Value |
|---|---|
| Journal | Advanced Theory and Simulations |
| Published | 2026-02-01 |
| Authors | R. Yamazaki, Jan Isberg, Nattakarn Suntornwipat, Saman Majdi |
| DOI | 10.1002/adts.202502259 |
A two-band Monte Carlo model matched hole drift in CVD diamond measured by time-of-flight at 80 K and 300 K. The model included heavy-hole and light-hole bands, acoustic scattering within and between them, and optical scattering within each band. Its fitted acoustic deformation potential was 10.10 eV. At 80 K and 5000 V/cm, interband scattering reduced the final heavy-hole population by about 21%.
Transport models locate the fitted deformation potential
Section titled “Transport models locate the fitted deformation potential”Earlier theory treated low-temperature hole transport with acoustic and optical phonon scattering inside a single heavy-hole band. This study extended the analysis to room temperature and included the light-hole band. Three models were tested at 80 K and 300 K over electric fields from 0 to 5000 V/cm.
| Model | Band treatment | Scattering mechanisms | Parameters used |
|---|---|---|---|
| 1 | Heavy hole | Intraband acoustic | (D_{ac}=9.00) eV |
| 2 | Heavy hole | Intraband acoustic and optical | (D_{ac}=9.00) eV, (D_{op}=2.45 \times 10^9) eV/cm |
| 3 | Heavy hole and light hole | Intraband acoustic and optical, interband acoustic | (D_{ac}=10.10) eV, (D_{op}=2.45 \times 10^9) eV/cm |
The acoustic-only model deviated most from measurements at high fields, where optical phonon scattering became dominant. Adding optical scattering brought the simulation into close agreement with the measurements. Models 2 and 3 showed no significant drift velocity difference. Model 2 was sufficient for a simple velocity prediction. Model 3 gave a more precise deformation potential and exposed band-specific dynamics.
The two-band fit returned 10.10 eV, compared with 9.00 eV used in single-band models. The fitted value is a model parameter, not a direct time-of-flight measurement.
Monte Carlo treatment of phonon scattering
Section titled “Monte Carlo treatment of phonon scattering”The simulation advanced each hole through a drift interval using a modified Newton’s law. It recalculated scattering rates, selected an event by the rejection technique, and updated energy and momentum. Acoustic absorption and emission changed hole energy continuously.
The optical phonon energy was 167 meV, and emission required the hole to exceed it. The interband acoustic heavy-hole to light-hole emission process had a stated threshold of 9.9 × 10⁻⁴ eV. The model used the same acoustic and optical deformation potentials for heavy and light holes. This was based on their shared fourfold-degenerate valence-band maximum. The approximation applies while hole states remain close to the Γ point.
For ensemble statistics, 600 holes were simulated independently. Current was accumulated from 0 to 80 ns in 1000 bins. The time of flight came from the pulse start and end times. Drift velocity was the sample thickness divided by that interval.
Time-of-flight measurement conditions
Section titled “Time-of-flight measurement conditions”The experimental material was electronic-grade CVD diamond, 390 micrometers thick with a 5 × 5 mm area. Its impurity concentration was below 1 × 10¹³ cm⁻³.
Before fabrication, the sample was boiled in HNO₃:H₂SO₄:HClO₄ at a 1:1:1 ratio for 40 minutes at 180 °C. It was then oxygen-terminated in oxygen plasma for 60 seconds. A semitransparent Ti/Al top contact had thicknesses of 15/200 nm and provided optical access.
Electron-hole pairs were generated with a 213 nm laser pulse lasting 800 ps at 713 Hz. The 5.82 eV photons exceeded the 5.47 eV diamond bandgap, limiting absorption depth to a few micrometers. The top contact received 50 micrometer bias pulses up to 200 V at 80 K and 300 K. Back-contact current was measured with a 1 GHz bandwidth, 24 dB gain amplifier.
Heavy-hole dominance and band redistribution
Section titled “Heavy-hole dominance and band redistribution”Heavy holes dominated total transport despite stronger interband rates for light holes. This occurred because other scattering mechanisms contributed more to heavy holes. The effective masses were 0.667 m₀ for heavy holes and 0.261 m₀ for light holes.
Light holes gained energy faster from the field, which promoted optical phonon emission. Optical emission removed excess energy, which weakened light-hole to heavy-hole transfer. Heavy holes changed momentum less, so heavy-hole to light-hole interband scattering remained relatively strong.
At 80 K and 5000 V/cm, the simulated final light-hole population rose as the heavy-hole population fell by about 21%. A redistribution also appeared below 500 V/cm. The authors linked this low-field effect to light-hole carriers gaining energy more readily through phonon absorption.
At 300 K, simulated initial and final populations differed only slightly because thermal energy already populated a broad range of states. Scattering rates were generally higher at 300 K because phonon occupation increased. The modeled occupation factor was 2.99 × 10⁻¹¹ at 80 K and 1.56 × 10⁻³ at 300 K.
Optical phonon absorption was nearly zero at 80 K, but emission occurred at 80 K. The authors attributed weak absorption to the very small optical phonon population.
High-field energy relaxation
Section titled “High-field energy relaxation”The average-energy analysis extended simulations to 10 kV/cm. At 10 V/cm, models 1 and 2 held average hole energies near 9.9 meV at 80 K. At 300 K, the corresponding values were 35.1 and 35.8 meV, respectively. These were close to thermal references of 10.3 meV at 80 K and 37.9 meV at 300 K. Acoustic scattering therefore kept carriers close to thermal equilibrium under weak fields.
In model 3, heavy-hole and light-hole mean energies were 8.9 and 8.6 meV at 80 K. At 300 K, the respective means were 33.8 and 33.3 meV under the same 10 V/cm field. The authors attributed this reduction to energy exchange between heavy-hole and light-hole states.
Near 2000 V/cm, models 2 and 3 reached the streaming-motion energy of 55.6 meV. Above that region, average energies followed the paper’s quasielastic trend. The associated critical field was 2.18 × 10⁵ V/cm.
Light holes entered the quasielastic regime at lower fields because their smaller mass supported faster acceleration. Heavy holes required higher fields before optical phonon emission controlled their energy. Optical phonon emission was the main cooling mechanism in the high-field regime. At 80 K, heavy-hole energy dropped above 2000 V/cm when optical emission was included.
Model limits and device implications
Section titled “Model limits and device implications”The authors list several limits on the model’s quantitative use.
- The split-off band was excluded, although it lies about 13 meV from the heavy-hole and light-hole maxima.
- The split-off band may affect transport at high temperature or under strong electric fields.
- Identical heavy-hole and light-hole deformation potentials become less reliable when holes move far from Γ.
- Ionized and neutral impurity scattering was omitted, so the fitted deformation potential may partly absorb their effect.
- The sample’s impurity concentration was extremely low, which the authors expected to keep this effect negligible.
- The framework is best suited to qualitative insight and regimes where its assumptions remain valid.
Because boron is the most common diamond acceptor, the results are relevant to boron-doped diamond devices. For device engineering, high-field drift models should include optical phonon emission and heavy-hole to light-hole transfer. The measured agreement supports that treatment for low-impurity CVD diamond at 80 K and 300 K. The tested field range reached 5000 V/cm.
The fitted 10.10 eV was obtained for the stated low-impurity sample and model, not for boron-doped diamond. Impurity scattering should therefore be included when extending the model to boron-doped devices.
Materials and support
Section titled “Materials and support”The study requires a 390 micrometer thick, 5 × 5 mm electronic-grade CVD diamond plate for optical time-of-flight measurements. 6CCVD’s diamond materials catalog includes MPCVD-grown single-crystal and polycrystalline plates and wafers with thicknesses from 0.1 to 500 micrometers, plus Ti metallization. Custom fabrication needs for the optical-access contact can be reviewed through engineering support.
View Original Abstract
ABSTRACT Understanding the charge carrier properties and the effects of local scattering mechanisms in semiconductor materials is essential to realize reliable electronic devices. In this study, Monte Carlo simulations on hole transport in diamond were performed including multiple scattering mechanisms and the results are compared with experimental data observed by hole time‐of‐flight (ToF) measurements. By incorporating interband scattering, the deformation potential for acoustic phonon scattering was extracted. Furthermore, the redistribution of the heavy and light hole populations was recorded, and their dynamic behavior was analyzed. Moreover, detailed analysis uncovered distinct transport behaviors under complex scattering mechanisms, predominantly driven by optical phonon interactions, consistent with experimental observations.
Boron Doped Single Crystal Diamond Plate
View Specs →
Single Crystal Cvd Diamond Plate
View Specs →
Customized Single Crystal Cvd Diamond Plate
View Specs →References we cover
Section titled “References we cover”- Carrier Scattering Mechanisms - Identification via the Scaling Properties of the Boltzmann Transport Equation
- Three-dimensional charge transport mapping by two-photon absorption edge transient-current technique in synthetic single-crystalline diamond