Controlling quantum spin coherence using a microscopic metallic structure
Paper details
Section titled “Paper details”| Field | Value |
|---|---|
| Journal | Applied Physics Express |
| Published | 2026-03-01 |
| Authors | Shintaro Nomura, Hideyuki Watanabe, Susumu Sasaki, Satoshi Kashiwaya |
| DOI | 10.35848/1882-0786/ae538c |
A shorted coaxial termination produced a 230 μs slow component in Hahn echo decay near a 10 μm Ti/Au wire. The reference diamond chip without the wire gave 24.3 μs. The wire also raised the Hahn echo signal above the reference at delays longer than 70 μs. These results show that a cable termination can change NV-center coherence by shaping the local electromagnetic environment.
Control through a reflected microwave current
Section titled “Control through a reflected microwave current”The authors changed the electromagnetic boundary condition around shallow nitrogen-vacancy centers instead of changing diamond growth or surface treatment. They mounted a Ti/Au wire tapered to a central width of 10 μm on a silicon substrate. An impedance-matched microstrip line connected it to a 305 mm RG174/U coaxial cable. They left the distal end open or shorted and terminated the other PCB end with 50 Ω. The cable carried an induced alternating current. The current returned as a reflected current. Open and short terminations produced phase shifts of 0 and π, respectively. Interference between the reflected and directly induced currents changed the local microwave field. At 1.85 GHz, the cable had an effective wavelength of 109 mm with a 67% wavelength reduction factor. Thus, the 305 mm cable represented about 2.8 effective wavelengths. PCB and silicon microstrip lines and connectors added to the total path length. Earlier work by the authors used Rabi oscillation imaging to map the near field around a micrometer-scale metal wire. The present experiment connects that field control to Hahn echo coherence and low-frequency RF switching.
Diamond sample and measurement setup
Section titled “Diamond sample and measurement setup”The sample was a 2.0 × 2.0 mm² (100)-oriented ultrapure electronic-grade diamond chip. The authors grew a 15 nm layer of 15N-doped, isotopically purified 12C diamond by microwave plasma-assisted chemical vapor deposition. The reported isotopic purity was 99.999%. They implanted He+ ions to increase NV-center formation. The chip was annealed in Ar/H2 at 1000 °C for 1.5 h. They then performed an air anneal at 450 °C for 24 h. The NV density on a chip without the Ti/Au structure was estimated at 0.6 ppm from NV-NV spin interactions. They mounted the diamond chip above the 10 μm wire. Microwave pulses came from an arbitrary waveform generator and local oscillator through a double-balanced mixer. A planar ring antenna irradiated the structure, while permanent magnets oriented the bias field along [111]. NV centers were excited with 520 nm laser pulses. A 50× objective with 0.55 NA and a scientific CMOS camera collected photoluminescence images. They used spatial imaging because the wire changed the microwave field near each center.
Rabi oscillation control at 1.85 GHz
Section titled “Rabi oscillation control at 1.85 GHz”The authors measured Rabi oscillations in a 1.3 × 4.0 μm² region 2.2 μm beneath the wire edge at 36 mT. The shorted termination gave 16.2 MHz, while the open termination gave 30.4 MHz. A reference chip on silicon without the Ti/Au structure gave 3.5 MHz. The corresponding local field ratios were 4.6 and 8.7. The termination therefore controlled the microwave amplitude seen by the NV ensemble. The stronger local field also damped the Rabi oscillations more strongly. The authors attribute this damping mainly to increased microwave noise. They attributed baseline and contrast changes to conversion between unstable negatively charged NV centers and neutral NV centers in shallow centers.
Hahn echo separates fast and slow relaxation
Section titled “Hahn echo separates fast and slow relaxation”Phase-cycled Hahn echo sequences canceled common-mode noise and baseline drift. At 36 mT, the Zeeman shift was about 1 GHz, which satisfied the frequency-selective condition for one NV orientation. The reference chip had T₂ = 24.3 μs, with fit bounds of +0.6/-0.7 μs. The shorted case produced a biexponential decay. Under the shorted termination, the fast component was 32 μs and the slow component was 230 μs. The reported fit bounds were +10/-25 μs for the fast component and +40/-70 μs for the slow component. With the cable open, the components were 14 μs and 26 μs, with fit bounds of +3/-4 μs and +8/-19 μs. The open case did not extend the decay beyond the reference. Both wire configurations produced smaller initial echo signals than the reference chip. The authors associate this early loss with increased high-frequency RF noise from extrinsic relaxation mechanisms. However, the shorted configuration exceeded the reference echo signal at delays longer than 70 μs. The authors interpret this longer echo as suppression of low-frequency RF noise. The Hahn echo probes RF frequencies from several kHz to around 1 MHz. Surface spin noise can induce current in the nearby wire and couple it to the cable termination. At those RF frequencies, the cable was much shorter than the wavelengths, so propagation phase shift was negligible. They suggest that the termination mainly changed the phase of reflected RF noise.
Spatially local RF control and signal switching
Section titled “Spatially local RF control and signal switching”The suppression was spatially short ranged. At 1.9 μm outside the wire, the shorted case gave T₂ = 23 μs and the open case gave 9 μs. Each profile had a single exponential decay. The Rabi frequencies in the inside and outside regions differed by less than 7%. The authors use this contrast to support a local origin for the RF-noise control. The same structure also switched a low-frequency RF signal on and off. They measured an XY4-6 sequence at 27 mT in a 1.3 × 26.2 μm² region under the wire edge. They chose the XY family because it partly compensates pulse imperfections under spatially varying microwave amplitude. A signal appeared near τ = 0.44 μs, corresponding to 1.1 MHz, for the open termination. It was strongly suppressed for the shorted termination. The authors tentatively attribute the signal to proton NMR from oxonium ions adsorbed on the diamond surface. They state that standard electromagnetic modeling agrees with the result. A detailed theoretical treatment is still needed to explain the switching fully.
Fabrication limits and engineering path
Section titled “Fabrication limits and engineering path”Residual reflections arise from imperfections at the SMA connector and wiring between the PCB and silicon pads. The authors had not fully controlled the total effective electrical length. It included the PCB microstrip, silicon wiring, and coaxial cable. The mechanical mount provided insufficient adhesion between the diamond chip and the silicon-supported wire. Substrate warping and particulate contamination can compromise that interface. The authors anticipate direct lithographic fabrication of the wire on the diamond to improve control and reproducibility. The present minimum wire width was 10 μm. They expect thinner wires to couple more strongly to the spin-noise source. The demonstrated coherence-control effect is confined to the low-frequency regime. Improved fabrication may extend control to higher frequencies, but the authors present this as a possibility.
Materials and support
Section titled “Materials and support”The device needs a 2.0 × 2.0 mm² (100)-oriented chip with a 15 nm 15N-doped, isotopically purified 12C layer, He+ implantation, and Ti/Au conductors. They annealed the implanted chip in Ar/H2 at 1000 °C for 1.5 h, then in air at 450 °C for 24 h. 6CCVD’s diamond materials catalog lists MPCVD-grown single-crystal and polycrystalline diamond, while engineering support can assess the 15 nm layer against the listed minimum thickness.
View Original Abstract
Abstract Increasing the coherence time of qubits is essential for enhancing the sensitivity of quantum sensors. For diamond nitrogen-vacancy centers, spin coherence times T 2 have primarily been extended through optimizing material preparation techniques such as crystal growth condition and surface treatment. Here, we demonstrate an alternative approach in which T 2 is tailored by engineering the local electromagnetic environment. By adjusting the termination conditions of a micrometer-scale metal wire placed near the diamond, we successfully controlled the microwave Rabi frequency and T 2 . Our findings highlight the potential of micrometer-scale metallic structures as a means to externally engineer and enhance quantum coherence.
Electronic Grade Intrinsic Diamond Epitaxial Wafer H Terminated Superior 100 Mosfet Ready Substrate
View Specs →
High Concentration Quantum Grade Single Crystal Diamond
View Specs →
Boron Doped Single Crystal Diamond Plate
View Specs →References we cover
Section titled “References we cover”- Wide-Field Dynamic Magnetic Microscopy Using Double-Double Quantum Driving of a Diamond Defect Ensemble
- Decoherence of ensembles of nitrogen-vacancy centers in diamond
- Sensitivity optimization for NV-diamond magnetometry
- System for the remote control and imaging of MW fields for spin manipulation in NV centers in diamond
- High density nitrogen-vacancy sensing surface created via He+ ion implantation of 12C diamond
Original source
Section titled “Original source”References
Section titled “References”- 2017 - Quantum sensing [Crossref]
- 2020 - Sensitivity optimization for nv-diamond magnetometry [Crossref]
- 2017 - Dynamics of non-markovian open quantum systems [Crossref]
- 2011 - An open-system quantum simulator with trapped ions [Crossref]
- 2000 - Quantum feedback control and classical control theory [Crossref]
- 2008 - How to enhance dephasing time in superconducting qubits [Crossref]
- 2010 - Robust decoupling techniques to extend quantum coherence in diamond [Crossref]
- 2010 - Universal dynamical decoupling of a single solid-state spin from a spin bath [Crossref]
- 2011 - Measurement of the noise spectrum using a multiple-pulse sequence [Crossref]