Local nanoscale probing of electron spins using NV centers in diamond
Paper details
Section titled “Paper details”| Field | Value |
|---|---|
| Journal | Diamond and Related Materials |
| Published | 2026-03-10 |
| Authors | Sergei Trofimov, Christos Thessalonikios, Victor Deinhart, Alexander Spyrantis, Lucas Tsunaki |
| DOI | 10.1016/j.diamond.2026.113530 |
| Citations | 1 |
Focused helium implantation created local NV ensembles that measured substitutional nitrogen at 234 ± 13 ppb in type IIa HPHT diamond. The measured sector was {111}, with an estimated 5 ppb detection limit and submicron spatial resolution.
Why local nitrogen matters
Section titled “Why local nitrogen matters”Substitutional nitrogen atoms, called P1 centers, supply the nitrogen needed to create NV centers. Their electron spins also generate magnetic noise that shortens NV coherence times.
Bulk measurements can miss sector-scale variation. Infrared C-center absorption has a detection limit near 1 ppm, while ultraviolet absorption reaches about 100 ppb. Both methods have spatial resolution on the order of tens of microns. EPR can detect nitrogen down to 1 ppb, but quantitative local measurements remain difficult.
HPHT diamond can show an order-of-magnitude nitrogen variation within one crystal. Here, the sensing volume is controlled by ion straggle and vacancy diffusion rather than only optical diffraction.
Diamond sample and growth sectors
Section titled “Diamond sample and growth sectors”The specimen was a (001)-oriented 3 mm × 3 mm × 0.37 mm single-crystal plate cut from type IIa diamond. It was grown at 5 GPa and 1750 K using a temperature-gradient HPHT process, then mechanically polished to Ra < 5 nm.
UV luminescence distinguished the {111}, {001}, and {113} growth sectors. Typical concentrations for comparable material were about 500 ppb in {111} and below 50 ppb in {001}. Quantitative EPR gave an average of 22 ppb for the sample. Under the assumption that other sectors contained at least ten times less nitrogen, this average implied about 80 ppb in {111}.
Confocal microscopy found no detectable single NV centers before implantation. PL saturation measurements after implantation gave an inferred P1 ratio of 10.1:1.3:1.0 for {111}:{113}:{001}. This estimate assumed that photoluminescence was proportional to nitrogen.
Writing local NV probes
Section titled “Writing local NV probes”Helium ion microscopy created the local probes with 30 keV helium ions. Doses ranged from 5 to 5000 ions per spot. SRIM predicted an average of 37 vacancies per ion, with the depth distribution peaking at about 120 nm. The focused beam set the starting damage site, while ion straggle and vacancy diffusion set the effective probe volume.
The plate was annealed in argon at 7 mbar. The schedule comprised 1 hour at 400°C, 1 hour ramping to 990°C, 2 hours at 990°C, and 2 hours cooling. Unfocused neutral atoms produced a circular bright feature about 60 µm across at every implantation site.
DEER measurement and extraction
Section titled “DEER measurement and extraction”The homebuilt confocal microscope used a permanent magnet to provide B0 ≈ 37 mT along one <111> NV family. NV and P1 transitions were driven at approximately 1.8 GHz and 1 GHz, respectively. A green continuous-wave laser and 0.95 NA objective provided excitation and photoluminescence collection.
DEER added a target-frequency microwave pulse to a Hahn echo sequence. When the pulse matched a P1 transition, the target spin shifted the NV phase and changed the NV photoluminescence. Five P1 peaks appeared with this field alignment, rather than 12 for other orientations. The central peak was excluded from nitrogen analysis because other g ≈ 2 electron spins could contribute there. The final nitrogen value averaged results from four remaining P1 peaks.
The fitting protocol used three steps. First, a frequency sweep located the resonance peaks. Second, Rabi oscillations measured the Rabi frequency and pulse length separately for each peak. Third, a second spectrum was fitted with the Rabi frequency fixed and target concentration free.
QuaCCAToo simulated the full laboratory-frame spin evolution without the rotating wave approximation. Simulations used g = 2 for NV, P1, and defect X, with spin 1/2 for the target P1 and X spins. The P1 measurements used TA = 20 µs, selected from the measured coherence time and 13C modulation.
Off-axis NV measurements used the |2⟩ ↔ |3⟩ transition, with TA = 80 µs. Simulations gave |σNV| = 0.87 and assigned the observed transition to 45% of all NV centers.
The estimated P1 limit was 5 ppb. It assumed 5% DEER contrast, TB = 0.35T2 ≈ 100 µs, and Rabi frequency much larger than the linewidth. This was an estimate rather than a concentration confirmed against a reference sample.
Nitrogen and implantation defects
Section titled “Nitrogen and implantation defects”Across 35 to 5000 ions per spot, the average P1 concentration in {111} was 234 ± 13 ppb. The paper describes this result as agreeing with the growth-based estimate of about 80 ppb. That earlier estimate depended on the tenfold lower nitrogen assumption.
The P1 values varied with implantation dose. The authors list P1 conversion into NV and X centers and local nitrogen variation as possible causes. Thus, each DEER value describes the implanted volume rather than a bulk average.
At 50 and 250 ions per spot, the additional central-line shoulder fell within measurement scatter. It became detectable at 1000 ions per spot and increased at 5000 ions per spot. Defect X reached up to 15 ppb, depending on implantation dose.
A simulation at 5000 ions per spot used 200 ppb P1 and 13 ppb X to reproduce the measured shoulder. The authors considered WAR10, a proposed interstitial nitrogen and carbon pair, but did not identify X conclusively. Adding a spin 1/2 Hamiltonian reproduced the additional resonance.
NV yield and vacancy diffusion
Section titled “NV yield and vacancy diffusion”The off-axis NV DEER signal increased with helium dose from 50 to 2500 ions per spot. PL saturation curves gave the same qualitative dose dependence. Dividing measured NV counts by their concentration gave VNV = (4.8 ± 0.3) × 10⁻² µm³. Assuming a spherical volume gave a radius of 226 ± 13 nm.
SRIM gave a vacancy radius of 37.5 nm, so the inferred diffusion length was 223 ± 13 nm. Using an annealing time of 7200 s yielded Dvac = 1.2 ± 0.1 nm²/s. The paper compares this with 1.8 nm²/s at 850°C and 1.1 nm²/s at 750°C from prior work.
The {111} ensemble had an average T2 of 284 ± 14 µs. At a 5000-ion site, the measured value was 313 ± 5 µs. Values above 100 µs approached the limit imposed by natural 13C at 1.1% abundance. This supports nitrogen below 1 ppm, although it does not resolve the 234 ppb local value.
Limits and implications
Section titled “Limits and implications”The P1 central resonance was not detected in {113}, even though the sector ratio implied about 20 ppb. PL-derived NV counts may have been overestimated because other luminescent defects, including NV0, were present. Fewer created NVs also increased the averaging time required for DEER.
Measurements were not performed in {001} because its estimated NV yield was close to {113}. Only the {111} sector received a direct quantitative P1 measurement. The other sectors were inferred to lie near the estimated 5 ppb limit rather than being directly quantified.
The method is not passive because implantation creates both the NV sensors and implantation-related defects. Extra single NVs also appeared between written sites, and their origin remained unclear. The 60 µm neutral-atom feature further shows that beam writing needs process control.
Material selection based only on a bulk nitrogen value can therefore miss the local sector variation in HPHT diamond. Device engineers should account for growth sector, implantation dose, annealing, and the resulting defect population when preparing NV sensors.
Materials and support
Section titled “Materials and support”The paper needs a polished type IIa HPHT single-crystal plate with low nitrogen for local NV ensembles and DEER measurements. The 6CCVD diamond materials catalog offers MPCVD single-crystal plates up to 125 mm and 0.1 to 500 µm thick, with Ra below 1 nm. The size and finish cover the plate, but HPHT growth and sector nitrogen are unconfirmed, so use the engineering support service to check low-nitrogen suitability.
View Original Abstract
Substitutional nitrogen atoms in a diamond crystal (P1 centers) are, on one hand, a resource for creation of nitrogen-vacancy (NV) centers, that have been widely employed as nanoscale quantum sensors. On the other hand, P1’s electron spin is a source of paramagnetic noise that degrades the NV’s performance by shortening its coherence time. Accurate quantification of nitrogen concentration is therefore essential for optimizing diamond-based quantum devices. However, bulk characterization methods based on optical absorption or electron paramagnetic resonance often overlook local variations in nitrogen content. In this work, we use a helium ion microscope to fabricate nanoscale NV center ensembles at predefined sites in a diamond crystal containing low concentrations of nitrogen. We then utilize these NV-based probes to measure the local nitrogen concentration on the level of 230 ppb (atomic parts per billion) using the double electron-electron resonance (DEER) technique. Moreover, by comparing the DEER spectra with numerical simulations, we managed to determine the concentration of other unknown paramagnetic defects created during the ion implantation, reaching 15 ppb depending on the implantation dose. • Nanoscale NV ensembles fabricated in HPHT diamond using helium ion microscope. • Local nitrogen concentration measured down to 230 ppb by NV-DEER technique. • Unknown paramagnetic defect X is detected by comparing DEER spectra with simulations. • Defect X confirmed to be implantation-related and quantified at the ppb level. • Volume occupied by NV ensembles determined, and vacancy diffusion length estimated.
Single Crystal Cvd Diamond Plate
View Specs →
Boron Doped Single Crystal Diamond Plate
View Specs →
Customized Single Crystal Cvd Diamond Plate
View Specs →References we cover
Section titled “References we cover”- Digital Twin Simulations Toolbox of the Nitrogen‐Vacancy Center in Diamond
- NV centres by vacancies trapping in irradiated diamond - experiments and modelling
- Decoherence of nitrogen-vacancy spin ensembles in a nitrogen electron-nuclear spin bath in diamond
- Rapid determination of single substitutional nitrogen Ns concentration in diamond from UV-Vis spectroscopy
- Determination of local defect density in diamond by double electron-electron resonance
Citing papers we cover
Section titled “Citing papers we cover”Original source
Section titled “Original source”References
Section titled “References”- 2020 - Nitrogen in diamond [Crossref]
- 2008 - High-sensitivity diamond magnetometer with nanoscale resolution [Crossref]
- 2011 - Electric-field sensing using single diamond spins [Crossref]
- 2013 - High-precision nanoscale temperature sensing using single defects in diamond [Crossref]
- 2006 - Room-temperature manipulation and decoherence of a single spin in diamond [Crossref]
- 2020 - Decoherence of ensembles of nitrogen-vacancy centers in diamond [Crossref]
- 2022 - Decoherence of nitrogen-vacancy spin ensembles in a nitrogen electron-nuclear spin bath in diamond [Crossref]
- 1990 - Growth-sector dependence of optical features in large synthetic diamonds [Crossref]
- 2013 - The origin of color in natural C center bearing diamonds [Crossref]