Calculation of characteristics of subnanometer delta-doped layers in diamond in the quasi-classical approach
Paper details
Section titled “Paper details”| Field | Value |
|---|---|
| Journal | Nanosystems Physics Chemistry Mathematics |
| Published | 2026-07-18 |
| Authors | V. A. Kukushkin, Yu. V. Kukushkin |
| DOI | 10.17586/2220-8054-2026-17-3-291-296 |
The quasi-classical calculation estimates the characteristics of an equilibrium boron delta-doped layer with less than 2% relative error for the stated 300 K case. It avoids solving the Schrödinger equation for hole states. The model treats a 0.1 nm boron monolayer with a sheet concentration of 3 × 10^13 cm^-2 in diamond containing 10^15 cm^-3 background boron. If an external field fully ionizes the layer, the same method gives estimates with less than 60% relative error.
Model scope and inputs
Section titled “Model scope and inputs”The target is an idealized, heavily boron-doped monolayer at x = 0, embedded in lightly doped CVD diamond with unintentional background boron. The surrounding concentration represents residual boron in the growth reactor. The thinnest reported boron delta-doped layers have thicknesses of order 1 nm, while the reported maximum doping abruptness is 1 decade/nm. The modeled monolayer therefore sits below the demonstrated layer thickness.
| Model input | Value |
|---|---|
| Boron sheet concentration, Nb | 3 × 10^13 cm^-2 |
| Monolayer thickness | of order 0.1 nm |
| Background boron concentration, Nbv | 10^15 cm^-3 |
| Temperature | 300 K |
| Boron activation energy, E0 | 370 meV |
| Spin-orbit splitting, Eso | 6 meV |
| Static permittivity | approximately 5.7 |
Quasi-classical calculation method
Section titled “Quasi-classical calculation method”The model solves the Poisson equation along x, normal to the layer, for a two-dimensional sheet. It combines the hole density, negatively charged background boron, and the boron sheet charge. The chemical potential is set to zero, and the valence-band edge follows Ev = Ev0 - eφ. Charge neutrality far from the layer fixes Ev0.
The equilibrium case uses a nondegenerate Maxwell-Boltzmann hole distribution. Its density of states uses heavy, light, and spin-split-off hole masses of 0.427m, 0.366m, and 0.394m, where m is the free electron mass. Negatively charged background boron follows the paper’s standard ionization relation. The potential is symmetric about x = 0, tends to zero away from the layer, and satisfies a field-jump condition at the sheet.
The equilibrium equations have an analytical solution for the potential and three-dimensional hole concentration. The fully ionized case requires a numerical solution with Fermi-Dirac hole distributions. A conventional treatment would jointly solve the Schrödinger and Poisson equations for quantized levels and wavefunctions. The quasi-classical method avoids those quantum-state calculations.
Equilibrium result and accuracy
Section titled “Equilibrium result and accuracy”The analytical equilibrium profile shows that only Nb- ≈ 3.5 × 10^10 cm^-2 of the sheet boron is ionized at 300 K. This is about 0.1% of Nb. The small free-hole population keeps the electrostatic potential smooth in x.
The authors check both statistical assumptions. The minimum hole nondegeneracy ratio is about 8.9, above 1. The corresponding background-boron ionization ratio far from the layer is about 5.2, also above 1. The calculated quasi-classical parameter is about 0.02. Using the cited error criterion, the authors estimate a relative error below 2%. These checks support the equilibrium profiles within the reported accuracy.
Fully ionized layer in an external field
Section titled “Fully ionized layer in an external field”The field case assumes every boron atom in the sheet is ionized, so Nb- = Nb. Free holes retain spatial and energy distributions similar to the equilibrium case at ambient temperature. Near the layer, the hole gas is degenerate and is calculated with Fermi-Dirac functions. Far from the layer, the nondegenerate limit gives the same Ev0 as in equilibrium.
For Nb = 3 × 10^13 cm^-2, the central ratio [Ev0 - eφ(0)]/kBT is about 8.3. The hole gas is therefore degenerate at x = 0 and nondegenerate far away. This transition gives Nh a complex dependence on φ, which prevents an analytical solution. The solution is obtained numerically.
The reported local wavelength variation is below 0.6, meeting the order-of-magnitude quasi-classical criterion without much margin. The estimated relative error is below 60%, so the field-ionized profiles serve only as estimates. The potential is sharp near the sheet, but degenerate holes have high kinetic energy and short wavelengths. The authors note that ordinary semiconductors do not show the same balance because their impurity activation energies are much smaller.
Optical ionization and hole heating
Section titled “Optical ionization and hole heating”The practical case uses an electromagnetic field to ionize neutral boron in the sheet. The photon threshold is set at ħω above 584 meV, corresponding to a wavelength below 2.1 μm. This energy makes the final free-hole state at least half empty.
The ionization cross-section is of order 10^-16 cm^2. The authors estimate recombination with a cross-section of 1.77 × 10^-13 cm^2, a hole Fermi velocity of 2 × 10^7 cm/s, and a center hole concentration of 3.9 × 10^20 cm^-3. These values give a recombination rate of 1.4 × 10^15 s^-1. At ħω = 584 meV, the calculated intensity threshold is above 1.3 × 10^12 W/cm^2.
A fiber laser can deliver this intensity at a focal spot with a diameter of several microns. The authors require pulsed operation to avoid diamond damage. They also estimate the hole heating. For hole energies above twice the 165 meV optical-phonon energy, the authors use a quasimomentum and energy relaxation time below 3 fs. Field heating raises the energy at less than 90 erg/s, while optical-phonon emission removes it at 90 erg/s or more. The 165 meV optical-phonon scale keeps the hole energy of the same order as the calculated 214 meV scale near the layer.
Comparison with demonstrated structures
Section titled “Comparison with demonstrated structures”The paper reports a calculation rather than a device measurement. Its one-monolayer structure has not been created, so the authors cannot compare the calculated hole profile with capacitance-voltage measurements or other experimental data. The thinnest achieved delta-doped layers have thicknesses of order 1 nm. In earlier 1 nm structures, the hole mobility increase associated with delta doping was not obtained.
Several assumptions remain specific to the model. The equilibrium calculation uses the ideal 0.1 nm sheet, 300 K, 3 × 10^13 cm^-2 sheet concentration, and 10^15 cm^-3 background concentration. Its statistical assumptions pass the stated checks. The field calculation has an estimated relative error below 60%. The paper reports no fabricated transistor, measured mobility, or device speed. The modeled layer is thinner than achieved structures, while the 1 decade/nm abruptness limit places current fabrication close to the proposed profile.
Implications for device design
Section titled “Implications for device design”Diamond offers high thermal conductivity, electrical strength, chemical and radiation resistance, and a low thermal expansion coefficient. Pure diamond is insulating, while heavy doping increases carrier scattering and reduces mobility. A delta-doped sheet separates ionized boron from part of the hole population. The authors state that this can raise mobility relative to uniform doping at the same delta-layer concentration.
The model gives potential and hole-density profiles for this structure without solving the Schrödinger equation. That reduces the calculation burden for preliminary design of high-speed field-effect transistors. The equilibrium result is the more reliable case, with estimated error below 2%. The field-ionized case should guide initial estimates only because its estimated error is below 60%. A sequence of delta-doped layers may provide conductivity and mobility at the same time, but the paper presents this as a design suggestion. Experimental comparison remains necessary because the target monolayer and its mobility benefit have not been demonstrated.
Materials and support
Section titled “Materials and support”The application calls for boron delta-doped CVD diamond films for high-speed field-effect transistor design, with a 0.1 nm boron sheet embedded in diamond containing 10^15 cm^-3 background boron. 6CCVD’s diamond materials catalog includes boron-doped diamond and single-crystal or polycrystalline diamond grown by MPCVD, but the paper’s delta-layer thickness and profile remain separate process requirements. The engineering support service can be used to define the proposed device structure and check which material specifications can be matched before the delta layer is fabricated.
View Original Abstract
It is shown that subnanometer boron delta-doped layers characteristics in chemically vapor deposited diamond films can be calculated in the quasi-classical approximation both in equilibrium and in an external electromagnetic field ionizing doping boron atoms. The corresponding solutions are found, in the first case - analytically, in the second - numerically. The use of the quasi-classical approximation allows one to simplify significantly the mathematical modeling of diamond structures with subnanometer delta-doped layers, necessary for their application in nanoelectronics, for example in high-speed field-effect transistors.
Boron Doped Single Crystal Diamond Plate
View Specs →
Free Standing Boron Doped Diamond Pcd Film
View Specs →
Boron Doped Diamond Electrode On Niobium Bdd Nb Electrode
View Specs →References we cover
Section titled “References we cover”- Investigation of boron-doped delta layers in CVD diamond grown on single-sector HPHT substrates
- The investigation of boron-doped diamond absorbance spectrum