Makhtesh Ramon - A unique natural-resource complex of strategic, multi-component mineral raw materials in Southern Israel

FieldValue
JournalStratigraphy Petroleum Sedimentology Geochemistry
Published2026-10-31
AuthorsLev V Eppelbaum
DOI10.35714/ggistrat20260200026

More than 300 microdiamonds were recovered from western Makhtesh Ramon, Southern Israel, including five diamonds above 1 mm. The largest measured 1.35 mm along its longest axis, and another measured 1.20 mm. Eppelbaum’s 2026 synthesis combines these finds with unrounded indicator minerals and shallow magnetic bodies to propose a local diamondiferous source. The evidence supports further exploration, but it does not establish an economic kimberlite or lamproite pipe.

Makhtesh Ramon is a 40 km long erosional canyon about 8 km wide in the northern Negev. Its formation ended about 132 Ma, after which alkaline basaltic, gabbroic, and kimberlitic associations accumulated. Regional magmatism peaked near 120 Ma. This falls within the 125 to 63.5 Ma interval that the author links to peak kimberlite formation. Mt. Arod, an Early Cretaceous basanitic-nephelenitic volcano with a diatreme, provides a recognized diatreme-bearing volcanic center within the area. The proposed diamond source lies farther west. There, erosion removed much of the sedimentary cover and left shallow indicators in alluvium and exposed volcanic rocks.

Four regional measurements support the search model. Heat flow is about 35 mW/m², while the paper’s cited deposit reference sets commercial diamond regions below 40 mW/m². The Moho lies at 38 km, the Curie Point isotherm at 39 km, and the crystalline basement at 3.3 to 3.5 km depth. The basement exceeds 30 km in thickness.

Local airborne magnetic modeling produced near-surface bodies at 8 to 50 m depth with thin-bed and “inverse carrot” geometries. The survey used a 1,000 m flight altitude, 2,000 m line spacing, and removal of the IGRF. Magnetic gradients show ring structures. One anomaly previously modeled as a sill was reinterpreted as most consistent with a kimberlite pipe. Self-potential modeling places the upper edge of a buried target at 25 to 30 m. Na+ and Ba2+ maps trace a southwest to northeast fault and outline prospective drilling areas. These bodies are interpreted as possible kimberlite or lamproite pipes, not confirmed pipes.

Samples came from the 10 to 80 cm near-surface layer and from Lower Cretaceous Arod conglomerates and Middle Quaternary to recent alluvium. Operators concentrated them in a temporary base in Mizpe Ramon. Conventional gravity concentration was less effective because selected grains had similar size and weight but different densities. The authors therefore used an enhanced concentration procedure before optical, X-ray luminescence, magnetic, and electron-microscope examination.

Target minerals had often been redeposited under the arid climate and covered by hard shells. The final preparation used boiling 3HCl+HNO3 and HF solutions to remove those shells. About 100 representative minerals were examined with a JSM5300 scanning electron microscope. Polymineral fractions were checked with a Camscan-DV microscope and Link AN10000 energy-dispersive microprobe. The paper calls this stage preliminary, although the reported counts cover thousands of grains.

The first mineral group contains chromediopside, orange garnet, bright-crimson pyrope, picroilmenite, chromespinel, and olivine. It also includes moissanite, perovskite, anatase, corundum, titanomagnetite, and tourmaline. More than 15,000 grains occurred in 150 kg of concentrate. The reported pyrope, garnet, chromediopside, picroilmenite, ilmenite, and spinel grains were not smoothed. Most grains in the first group also showed no rounding or oxidation. The author treats these surfaces as evidence for nearby indigenous sources rather than long alluvial transport.

Electron microscopy found chromium, magnesium, and aluminum in pyrope, and cobalt, chromium, magnesium, and nickel in picroilmenite. The reported clinopyroxene chemistry includes 0.5 to 1.2% Cr2O3 and 2.5 to 6% FeO. It also includes 2.3 to 6.6% Al2O3 and 0.5 to 1.5% Na2O. These values place the grains in the paper’s chromediopside and kimberlite comparison fields. Coesite occurred in large volumes, and yttrium phosphate was also identified.

Petrographic work provides a separate line of evidence. The studied effusive rocks contain olivine, clinopyroxene, titanomagnetite, nepheline, and glass. Feldspars occur in some samples, and nepheline reaches 5 to 10%. K-Ar dating places the magmatic rocks at 125 to 115 Ma. One sample was classified as meimechite, and its composition was described as similar to kimberlite associations. The paper divides the effusive rocks into samples with and without plagioclase. The broader magmatic setting includes peridotite xenoliths, alkaline basalts, basanites, melilites, and alkaline picrites. These observations support deep volcanic involvement, but the meimechite classification does not identify a diamondiferous pipe.

The recovery count exceeded 300 microdiamonds below 1 mm. Five diamonds ranged from 1 to 1.35 mm along their longest axes. Most had cubic habits, while fewer were hexagonal. Table 1 lists the largest crystal at 1.35 x 1.15 x 0.75 mm, with a density of 3,510 kg/m³ and a mass of 4.09 mg. The authors describe the two largest crystals as fragments of a larger crystal.

The same work also detected small native gold plates, silver flakes, and traces of La, Ce, Th, Nb, and Ta. Earlier studies reported platinum-group elements near Makhtesh Ramon and in Makhtesh Gadol. These results support a separate polymetallic and rare-earth-element target, although the paper reports no assay values for the gold, silver, or rare-earth-element concentrations.

The author links the Makhtesh Ramon discovery with diamond and indicator-mineral reports from Qishon Valley, northwest Syria, and the Central Eastern Desert of Egypt. The resulting map defines an East Mediterranean to Nubian diamondiferous belt. Makhtesh Ramon chromediopsides also resemble the low-baric group from the Arkhangelskaya pipe. That group was interpreted as derived from disintegrated spinel peridotites. The local chromediopsides also resemble those associated with diamondiferous lherzolites and websterites in the Zolotnitsky field. These comparisons support the proposed mantle-related source, but they are mineralogical similarities rather than direct evidence of a diamond pipe.

Unresolved questions and exploration implications

Section titled “Unresolved questions and exploration implications”

The largest unresolved issue is source confirmation. No drilling result or measured pipe is presented. The candidate bodies remain interpretations of magnetic, self-potential, and ion-selective data. The mineral work is explicitly preliminary, with 1,459 grains measured from eight sites. No grade, tonnage, or economic resource estimate is given.

The author also assigns six positive indicators a probability of 1/2 each. This produces a 1.56% chance of random coincidence and a stated 98.44% positive assessment. That calculation assumes independent, equally weighted evidence, so it should be read as an exploration heuristic rather than a calibrated probability. Mining is also prohibited within the state geological reserve.

The data define a practical next step. Regional screening can focus on the shallow 8 to 50 m bodies, while sampling should retain both alluvial and exposed bedrock material. Until drilling and systematic mineralogical work confirm the source, the supported conclusion remains limited to a promising occurrence of more than 300 microdiamonds, five crystals above 1 mm, and fresh kimberlite indicator minerals in western Makhtesh Ramon.

View Original Abstract

An integrated analysis of regional geological and geophysical factors led to selecting the Makhtesh Ramon area (northern Negev, Israel) to search for diamondiferous associations.The most important regional factor is the Middle Cretaceous maximum in upper-mantle hot-spot development, which appears prominently in this area.Analysis of magnetic (paleomagnetic), self-potential, and ion-selective data unambiguously indicates the presence of some bodies possibly having kimberlite (lamproite) origin occurring at small depths (8-50 m) in the western Makhtesh Ramon.Repeated erosion in the area removed most of the sedimentary associations and significantly simplified mineral sampling and rock collection for geochemical and petrological analyses.Comprehensive mineralogical analyses enabled the detection of the following minerals-satellites of diamond associations: chrome-diopside, orange garnet, bright-crimson pyrope, picroilmenite, moissanite, corundum, black spinel, olivine, anatase, and tourmaline (including black samples).These minerals are not rolled or oxidized, providing additional evidence of their association with the indigenous rocks.Data from electron microscopy show that the grains of (1) picroilmenite and (2) pyrope contain, respectively: (1) cobalt, chrome, magnesium, and nickel and (2) chrome, magnesium, and aluminum.This indicates that both picroilmenite and pyrope have a hyper-abyssal origin, which also indicates the possible occurrence of diamondiferous pipes.Secondaryimportance satellite minerals include feldspars, pyroxenes, magnetite, hematite, ilmenite, galena, pyrite, limonite, mica, chromite, leucoxene, zircon, rutile, etc.These minerals (compared with the first group) also indicate diamond-bearing mineralization in the studied area.Small gold and silver plates, along with considerable traces of La, Ce, Th, Nb, and Ta (Rare earth elements), may also be associated with the nearest kimberlite rock occurrence.The total number of recognized microdiamonds exceeds 300; five diamonds (> 1 mm) were identified (the largest crystals are 1.2 and 1.35 mm).Thus, based on a set of geological-geophysical factors and the identification of the mentioned minerals, we estimate that the Makhtesh Ramon area is promising for discovering diamondiferous rocks (kimberlite or lamproite pipes) as well as diamond crystals in loose deposits.The discovered silver-, gold-, and REE-bearing signatures may be important on their own.