Four geological-genetic deposit classes account for most recognized primary diamond occurrences: kimberlitic, lamproitic, metamorphogenic, and impact-related. The strongest economic example is the Argyle lamproite pipe in Western Australia, which provides about 40% of global diamond production. The paper links this diversity to magma source, emplacement form, wall-rock contamination, later alteration, and, for some deposits, impact pressure.

The mantle-derived group includes kimberlites, lamproites, kimberlite-lamproites, picritic monchiquites, lamprophyres, komatiites, and garnet pyroxenites. Impactites form a crustal class created by cosmic-body impacts. Kimberlites, lamproites, and kimberlite-lamproites mainly occupy diatremes and dikes, with fewer stockworks and sills. Other primary deposits occur mainly as intrusive massifs or plutons.

Kimberlite and lamproite magmas carried fragments of peridotite and eclogite from the mantle into the crust. Lamproites contain more Ti, K, P, and several other elements than kimberlites. The comparison reports no significant difference between diamonds in these two magmatic rocks. This separates rock classification from crystal identity.

The paper is a synthesis rather than a controlled experiment. It compares field descriptions from Siberian, East European, South African, and Australian provinces, plus the Indian Majhgawan occurrence. The evidence includes pipe and dike geometry, vertical sections, petrography, mineral chemistry, whole-rock geochemistry, indicator-mineral abundance, radiometric ages, and diamond inclusions. Carbon isotope data and crystal morphology provide further checks on diamond origin.

Most mantle-derived deposits lie within ancient cratons consolidated by the Archean. The paper notes exceptions in Proterozoic mobile belts. The Argyle pipe lies in the King Leopold belt, while Venetia and River Ranch lie in the Limpopo belt. Their existence does not remove the broader craton-centered pattern.

Erosion controls the preserved shape more than age alone. The roughly 90-million-year kimberlites of the Kaapvaal craton have lost more than 1,000 m, while the 189.3-million-year Mwadui pipe was barely eroded. This contrast shows why crater, pipe, and root-zone observations cannot be treated as interchangeable.

A weakly eroded diatreme can preserve a crater, vertical channel, and root or feeder zone. The Arkhangelsk tuffogenic package extends down to 130 to 160 m and contains up to 12 interlayers of tuffs and tuffites. Individual interlayers are 0.3 to 10 m thick. Deeper parts shift from sedimentary-volcanic rocks to kimberlite tuffs, eruptive breccias, autolith breccias, and porphyritic kimberlite.

Vertical changes reflect both magma movement and wall-rock capture. With depth, kimberlite becomes cleaner of terrigenous carbonate material, while deep mantle xenoliths become more important. Secondary alteration generally weakens downward, although saline or hydrothermal systems can maintain intense alteration below 1 km. The contrast is clear in Arkhangelsk kimberlites, where saponite averages more than 50% of rock volume.

Diamond content varies within a single pipe. Preserved upper crater sedimentary-volcanic zones have two to three times lower diamond content than deeper units. In Angola, the content is six to 30 times lower. The maximum occurs in central autolith breccias, while contact zones are usually depleted. The same intrusion phase shows little change in diamond morphology or physical properties during transition into the feeder channel.

Crater facies contain the smallest crystals and the largest number of broken fragments. Arkhangelsk diamonds are divided into a group larger than 2 mm and a group smaller than 1 mm. Pyrope there typically remains at the level of the first grams per tonne of kimberlite breccia. Chromspinellid ranges from 10.5 to 91.8 g/t. High-chromium varieties contain 52 to 60% Cr2O3.

Lamproites and the kimberlite-lamproite boundary

Section titled “Lamproites and the kimberlite-lamproite boundary”

The Argyle pipe provides the clearest quantitative case. Its dike-like body is 2 km long, 150 to 500 m wide, and covers 50 ha. A cup-shaped body of non-sandy tuff reaches 200 m thickness and has a surface extent of 200 by 100 m. Later olivine-phlogopite lamproite dikes are usually less than 1 m thick.

Argyle diamond quality is low relative to gem expectations. Only 5% are high-quality gem stones, 40% are low-quality gems, and the remainder are technical grades. Within the pipe, sandy tuff has the highest diamond content, non-sandy tuff is intermediate, and final magmatic lamproite has the lowest. The author suggests that high-temperature oxidation at low pressure and high oxygen potential during emplacement may explain the depleted magmatic lamproite.

Majhgawan in India defines an intermediate kimberlite-lamproite. Sm-Nd and K-Ar isotope dating gives a Precambrian age of 940 million years. Its rock contains 0.46 to 1.79% K2O, lacks clinopyroxene and potassium richterite, and has few pyrope, picroilmenite, and chromite grains. This combination is closer to lamproite, but the lower potassium and missing minerals support an intermediate classification.

Kokchetav microdiamonds rarely exceed a fraction of a millimeter. Their cubic, skeletal, and aggregate habits formed under disputed pressure-temperature conditions. Some researchers place their formation in the mantle after subduction to about 150 km. Others propose crustal metasomatosis or contact with intrusions that generated ultrahigh pressures.

The impact alternative places formation in a solid-state conversion of graphite to diamond. Impact diamonds occur in meteorite craters and meteorites. Popigai is the main Siberian example. Its type XI material is polycrystalline and contains diamond, lonsdaleite, and graphite. Natural grains average about 0.1 mm, although Yakutite aggregates exceeding 1 mm occur in placers. The primary sources of Yakutite aggregates remain unknown and may not be unique.

Exploration and material-selection implications

Section titled “Exploration and material-selection implications”

Indicator-mineral suites cannot be transferred directly between cratons. Productive central Siberian pipes are mostly high-indicator-mineral kimberlites, productive Arkhangelsk pipes are low-indicator-mineral types, and most productive South African pipes belong to the high-indicator group. Their mineral chemistry also differs. Exploration should therefore combine local indicator-mineral ratios with pipe architecture, alteration, and xenolith distribution.

For diamond material selection, deposit class alone is insufficient. The paper records crystal size, habit, inclusions, breakage, carbon isotope data, and the share of technical grades. It reports no thermal, electrical, optical, wear, or device-level performance data. A technical specification cannot rank kimberlite, lamproite, metamorphogenic, or impact diamond by engineering performance from this paper alone.

Exploration for non-kimberlite sources should inspect ring structures and carbon-bearing rocks such as graphite, coal, and bitumen. The uncertain Yakutite sources show why carbon isotopes and crystal structure must be checked before assigning a placer to an impact deposit. Material selection should begin with the intended application and specify crystal size, morphology, inclusion state, and geological class.

View Original Abstract

Globally recognized types of diamond-bearing magmatites can generally be classified into two groups, the mantle-derived and crustal ones. The first group comprises kimberlites, lamproites, kimberlite-lamproites, picritic monchiquites, lamprophyres, komatiites, and garnet pyroxenites. The crustal rocks are represented by impactmetamorphogenic types, or impactites. There is currently no consensus regarding the genetic type of diamonds found in crystalline rocks (of the Kokchetav type): some researchers assign them to the mantle group, while others argue for the crustal origin. Kimberlites, lamproites, and kimberlite-lamproites typically occur as diatremes and dikes, and less frequently as stockworks and sills. Other types of primary diamond deposits are hosted in crustal rocks that mainly occur as intrusive massifs (plutons). The original source of kimberlites and lamproites is represented by disintegrated mantle rocks (peridotites and eclogites), which fragments were brought into the Earth’s crust by the magma. The lamproites differ from the kimberlites in their high content of Ti, K, P, and certain other elements. There are no significant differences between the diamonds found in these two types of magmatic rocks. Metamorphogenic diamonds from the crystalline complex are very small (rarely exceeding a fraction of a millimeter) and occur as crystals of cubic habit, skeletal forms, and their aggregates. They formed under crustal conditions at P-T parameters characteristic for stability of this mineral. A new type of primary diamond deposit, associated with impactites, formed as a result of an impact of cosmic bodies onto the Earth’s surface. The diamond crystallization in these deposits resulted due to the solid-phase transition of graphite to diamond under high pressures generated during the impact. Diamonds from kimberlites and lamproites are valuable for both gem and technical applications; the technical significance is characteristic of other diamond types as well.