3D Imaging on heterogeneous surfaces on laterite drill core materials
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2017-12-01 |
| Journal | Qucosa (Saxon State and University Library Dresden) |
| Authors | Henry PilliĆØre, T Lefevre, Dominique Harang, Beate Orberger, Thanh Q. Bui |
Abstract
Section titled āAbstractāThe SOLSA project aims to construct an analytical expert system for on-line-on-mine-real-time mineralogical and geochemical analyses on sonic drilled cores. A profilometer is indispensable to obtain reliable and quantitative data from RGB and hyperspectral cameras, and to get 3D definition of close-to-surface objects such as rheology (grain shape, grain size, fractures and vein systems), material hardness and porosities. Optical properties of minerals can be analyzed by focusing on the reflectance.\nPreliminary analyses were performed with the commercial scan control profilometer MI-CRO-EPSILON equipped with a blue 405 nm laser on a conveyor belt (depth resolution: 10 μm; surface resolution: 30x30 μm2 (maximum resolution; 1m drill core/4 min). Drill core parts and rocks with 4 different surface roughness states: (1) sonic drilled, (2) diamond saw-cut, polished at (3) 6 mm and (4) 0.25 μm were measured (see also abstract DuĆ©e et al. this volume). The ĪICRO- EPSILON scanning does not detect such small differences of surface roughness states. Profilometer data can also be used to access rough mineralogical identification of some mineral groups like Fe-Mg silicates, quartz and feldspars). Drill core parts from a siliceous mineralized breccia and laterite with high and deep porosity and fractures were analyzed. The determination of holesā convexity and fractures) is limited by the surface/depth ratio. Depending on end-userās needs, parameters such as fracture densities and mineral content should be combined, and depth and surface resolutions should be optimized, to speed up āon-line-on-mine-real- timeā mineral and chemical analyses in order to reach the target of about 80 m/day of drilled core.
Tech Support
Section titled āTech SupportāOriginal Source
Section titled āOriginal Sourceā- DOI: None