Responsivity Study of Diamond X-ray Monitors with nUNCD Contact
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2015-01-01 |
| Journal | JACOW |
| Authors | Mengjia Gaowei, E. Müller, J. Smedley, Anirudha V. Sumant, Tianyi Zhou |
| Institutions | Argonne National Laboratory, RIKEN BNL Research Center |
| Citations | 2 |
| Analysis | Full AI Review Included |
Responsivity Study of Diamond X-ray Monitors with nUNCD Contact: Technical Documentation
Section titled “Responsivity Study of Diamond X-ray Monitors with nUNCD Contact: Technical Documentation”Executive Summary
Section titled “Executive Summary”- Application: X-ray beam position monitors for synchrotron beamlines (0.2-28 keV photon range), developed at Brookhaven National Laboratory.
- Device Architecture: Symmetric diamond detector utilizing nitrogen-doped ultrananocrystalline diamond (nUNCD) as electrodes on both sides of a CVD single-crystal diamond substrate, replacing conventional platinum (Pt) contacts.
- Key Achievement: nUNCD contact demonstrated responsivity comparable to theoretical predictions (within 4% deviation), with successful charge collection at a lower bias of 50V versus the 100V required for Pt-contact devices.
- Performance Advantage: At the carbon K-edge (~284 eV), the nUNCD contact outperformed the Pt-contact detector due to significantly lower x-ray absorption (Pt M-edges cause spectral artifacts and signal loss).
- Substrate Specs: Electronic grade SCD (~ppb nitrogen), 4 mm × 4 mm × 0.3 mm, with 200-500 nm nUNCD layers grown via MPCVD.
- Characterization: Validated at three NSLS beamlines (U3C, X8A, X15A) under varying vacuum conditions and biasing modes (DC and square-wave duty cycles for electron detrapping).
Technical Specifications
Section titled “Technical Specifications”| Parameter | Value | Unit | Context |
|---|---|---|---|
| Substrate Material | Electronic Grade SCD | — | [N] ~ppb level purity |
| Substrate Dimensions | 4 × 4 × 0.3 | mm | Standard BNL test geometry |
| nUNCD Layer Thickness | 200 - 500 | nm | Grown via MPCVD at ANL |
| Fitted nUNCD Thickness | 480 | nm | Including dead carbon layer effect |
| Fitted Diamond Bulk Thickness | 380 | µm | Extracted from 4-6 keV tail fitting |
| Tested Photon Energy Range | 0.2 - 28 | keV | Multi-beamline validation |
| Bias Voltage (nUNCD) | 50 | V | For >95% charge collection |
| Bias Voltage (Pt reference) | 100 | V | Required for full carrier extraction |
| Mean Ionization Energy (W) | 13.6 | eV | 4% deviation from literature 13.3 eV |
| X-ray Attenuation Length (350 eV) | 0.0878 | µm | Diamond bulk, CXRO data |
| X-ray Attenuation Length (1 keV) | 1.2888 | µm | Diamond bulk, CXRO data |
| X-ray Attenuation Length (19 keV) | 7129.76 | µm | Diamond bulk, CXRO data |
| Minimum Transmission Energy | 1350 | eV | For full traversal of 300 µm diamond |
| Beam Intensity Range | 10-9 - 10-6 | W/mm2 | Incident beam calibration range |
| U3C Vacuum Level | 10-7 | torr | Low-energy soft x-ray beamline |
| X8A Vacuum Level | 10-6 | torr | Mid-range monochromatic beamline |
| Detector Biasing Modes | DC / Square Wave | — | With adjustable magnitude, frequency, and duty cycle |
Key Methodologies
Section titled “Key Methodologies”- Substrate Preparation: Electronic grade CVD single-crystal diamond (4 mm × 4 mm × 0.3 mm, ~ppb nitrogen) selected as bulk detector material.
- nUNCD Layer Deposition: Nitrogen-doped ultrananocrystalline diamond layers (200-500 nm) grown on both faces via MPCVD at Argonne National Laboratory using Ar/CH4/N2 plasma chemistry to achieve semi-metallic conductivity.
- Pre-Fabrication Characterization: X-ray white-beam topography at NSLS Beamline X19C and polarized-light birefringence imaging to verify crystal quality and identify slip bands.
- Multi-Beamline Validation:
- U3C: Monochromatic beam, 0.2-1 keV, 10-7 torr vacuum.
- X8A: Monochromatic beam, 1-6.5 keV, 10-6 torr vacuum.
- X15A: 6.5-28 keV, in-air configuration.
- Incident Power Calibration: Silicon photodiodes (25 µm at U3C, 52 µm at X8A); air-filled ionization chamber at X15A.
- Electrical Readout: DC and pulsed square-wave biases with tunable duty cycles applied for hole/electron collection and detrapping.
- Theoretical Modeling: Modified Beer-Lambert responsivity equation incorporating nUNCD filter thickness, dead carbon layer, and bulk diamond attenuation.
6CCVD Solutions & Capabilities
Section titled “6CCVD Solutions & Capabilities”Applicable Materials:
- Electronic Grade SCD (Optical Grade): The electronic grade single-crystal diamond substrate used here (~ppb nitrogen) is directly within 6CCVD’s MPCVD production scope, with thicknesses from 0.1 µm to 500 µm and dimensions scalable to 125 mm for polycrystalline formats.
- Ultrananocrystalline Diamond (UNCD) / nUNCD Layers: 6CCVD’s MPCVD platform can deposit nanocrystalline and ultrananocrystalline diamond films with tunable sp2/sp3 ratios. Nitrogen doping for semi-metallic conductivity is achievable through Ar/CH4/N2 plasma recipes.
- Boron-Doped Diamond (BDD): For alternative conductive contact schemes or bulk-conducting detector designs, heavy boron-doped polycrystalline diamond is available in thicknesses up to 500 µm.
Customization Potential:
- Tailored Thickness Control: The paper notes that nUNCD thickness variation (200-500 nm) creates non-uniform response maps at low energies (halo artifacts). 6CCVD offers precision thickness control and in-house metrology for sub-µm layer uniformity critical to detector-grade responsivity.
- Custom Metalization: For hybrid contact architectures (e.g., nUNCD + bonding pads), 6CCVD provides internal Au, Pt, Pd, Ti, W, and Cu metallization with customizable pad geometries and laser-cut form factors.
- Laser Cutting & Dicing: Custom shaping of 4 mm × 4 mm plates or wafer-scale substrates into detector geometries with tight dimensional tolerances.
Engineering Support:
- 6CCVD’s in-house PhD engineering team can collaborate on detector-grade diamond selection, including SCD purity grading, nUNCD conductivity optimization, and electrode interface engineering for synchrotron, medical imaging, and beam diagnostic applications.
- Available consultation on dead carbon layer mitigation, MPCVD growth parameter optimization, and bias-dependent charge collection modeling.
Call to Action:
For custom specifications, metallization stack design, or material consultation for your x-ray detector or beam diagnostics project, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract
Nitrogen doped ultrananocrystalline diamond (nUNCD) grown on the surface of a CVD single crystal diamond is tested at various beamlines covering an x-ray photon energy range of 200eV to 28 keV. The nUNCD has much lower x-ray absorption than metal contacts and is designed to improve the performance of our device. The responsivity of nUNCD diamond x-ray detector is compared with the conventional platinum coated diamond x-ray beam position monitor and the results are presented in this paper.