Simulation and test of Silicon-on-Diamond sensors for particle detection
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2015-06-01 |
| Authors | D. Passeri, A. Morozzi, L. Servoli, K. Kanxheri, S. Sciortino |
| Institutions | Istituto Nazionale di Fisica Nucleare, Istituto Nazionale di Fisica Nucleare, Sezione di Firenze |
| Citations | 1 |
Abstract
Section titled āAbstractāA laser bonding technique has been developed recently to create an innovative material based on a silicon/diamond interface. In this work, we propose the development and the application of a numerical model for TCAD simulations of poly-crystalline diamond conceived for Silicon-on-Diamond (SoD) sensors to be used, e.g., as particle detectors in High Energy Physics (HEP) experiments. The model is based on the introduction of an articulated, yet physically based, picture of deep-level defects acting as a recombination centers and/or trap states. The modelling scheme has been validated by comparing the simulation findings with experimental measurements carried out on real devices featuring a thinned CMOS Active Pixel Sensor chip bonded to a poly-crystalline diamond substrate. Eventually, this technique could foster the exploration of innovative semiconductor devices conjugating the properties of diamond substrates and the capabilities of CMOS electronics.