A Study on Residual Stresses in Machined Brittle Material
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2015-11-01 |
| Journal | Advanced materials research |
| Authors | Pei Lum Tso, Tsung Yun Tsai |
Abstract
Section titled āAbstractāResidual stresses in fused silica induced by two machining methods, diamond blade saw cutting and GC grinding wheel grinding, are studied in this study. Photoelastic method would be applied as measuring tool analyzing the gradient of residual stresses caused by different machining condition. This sentence is strange with analyzing the chips of grinding and observation of surface defects, it is assumed that the stresses gradient differs probably cause by the different material removal mechanism.