“Freeing” Graphene from Its Substrate - Observing Intrinsic Velocity Saturation with Rapid Electrical Pulsing
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2015-12-09 |
| Journal | Nano Letters |
| Authors | Harihara Ramamoorthy, Ratchanok Somphonsane, Joshua Radice, Guanchen He, C.-P. Kwan |
| Institutions | University at Buffalo, State University of New York, Chiba University |
| Citations | 48 |
Abstract
Section titled “Abstract”Rapid (nanosecond-scale) electrical pulsing is used to study drift-velocity saturation in graphene field-effect devices. In these experiments, high-field pulses are utilized to drive graphene’s carriers on time scales much faster than that on which energy loss to the underlying substrate can occur, thereby allowing the observation of the highest saturation velocities reported to date. In a dramatic departure from the behavior exhibited by conventional metals and semiconductors, as the electron or hole density is reduced toward the charge-neutrality point, the drift velocity is found to reach values comparable to the Fermi velocity itself. Corresponding current densities are as large as 10(9) A/cm(2), similar to the values reported for carbon nanotubes and for graphene-on-diamond transistors. In essence, our approach of rapid pulsing allows us to “free” graphene from the deleterious influence of its substrate, revealing a pathway to achieve the superior electrical performance promised by this material. The usefulness of this approach is not merely limited to graphene but should extend also to a broad variety of two-dimensional semiconductors.