Selective deposition of polycrystalline diamond films using photolithography with addition of nanodiamonds as nucleation centers
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2016-02-01 |
| Journal | IOP Conference Series Materials Science and Engineering |
| Authors | V. Okhotnikov, Stepan Linnik, A. V. Gaidaichuk, D V Shashev, G Yu Nazarova |
| Institutions | National Research Tomsk State University, Tomsk State University of Control Systems and Radio-Electronics |
| Citations | 4 |
Abstract
Section titled āAbstractāA new method of selective deposition of polycrystalline diamond has been developed and studied. The diamond coatings with a complex, predetermined geometry and resolution up to 5 [mu]m were obtained. A high density of polycrystallites in the coating area was reached (up to 32Ā·10{7} pcs/cm{2}). The uniformity of the film reached 100%, and the degree of the surface contamination by parasitic crystals did not exceed 2%. The technology was based on the application of the standard photolithography with an addition of nanodiamond suspension into the photoresist that provided the creation of the centers of further nucleation in the areas which require further overgrowth. The films were deposited onto monocrystalline silicon substrates using the method of āhot filamentsā in the CVD reactor. The properties of the coating and the impact of the nanodiamond suspension concentration in the photoresist were also studied. The potential use of the given method includes a high resolution, technological efficiency, and low labor costs compared to the standard methods (laser treatment, chemical etching in aggressive environments).