Skip to content

Improved fracture behavior and microstructural characterization of thin tungsten foils

MetadataDetails
Publication Date2016-06-20
JournalNuclear Materials and Energy
AuthorsV. Nikolić, Stefan Wurster, Daniel Firneis, Reinhard Pıppan
InstitutionsErich Schmid Institute of Materials Science, Austrian Academy of Sciences
Citations20

This study is focused towards the development of the technique for investigating the fracture behaviour of 100µm thick rolled tungsten foils, with a purity of 99.97%. Electron backscatter diffraction (EBSD) scans reveal that the grains are elongated along the rolling direction of the foil, which has a very strong {100}<011> texture. The test specimens were fabricated by electrical discharge machining (EDM) and cracks were initiated by consecutively using a diamond wire saw, a razor blade and a focused ion beam (FIB) workstation. Fracture experiments were performed at temperatures from āˆ’196°C to 800°C. The investigation of fracture appearance shows an improved behavior and significantly higher values of conditional fracture toughness Kq compared to bulk W-materials, which can be related to a higher degree of deformation during the production process. A high toughness at room temperature (RT) and 200°C, slowly decreases when approaching the highest testing temperature of 800°C. The most significant result reveals that the ductile to brittle transition temperature (DBTT) is around RT, which is an extraordinary result for any tungsten material. The fracture surfaces, investigated with a scanning electron microscope (SEM), show a transition from cleavage fracture at liquid nitrogen temperature, through pronounced delamination within the foil plane at ambient temperatures to ductile fracture at the highest testing temperatures.