Quantum biomimetic modeling of magnetic field sensing using diamond NV−centers

MetadataDetails
Publication Date2016-08-01
AuthorsVishvendra Singh Poonia, Dipankar Saha, Swaroop Ganguly
InstitutionsIndian Institute of Technology Bombay
Citations1

A modeling framework, previously applied to magnetic field sensing in a quantum biological system, is extended here to study the optical and spin dynamics of the diamond nitrogen-vacancy (NV <sup xmlns:mml=“http://www.w3.org/1998/Math/MathML” xmlns:xlink=“http://www.w3.org/1999/xlink”&gt;-&lt;/sup> ) center. This points the way towards diamond-based precision magnetometry.