Investigation of the thermal mode in the composite diamond-bearing material in a polymer matrix
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2016-10-01 |
| Authors | Martin M. Yakhutlov, Umar D. Batyrov, Marianna R. Kardanova, Astemir A. Gutov, Zalim N. Deunezhev |
| Institutions | Kabardino-Balkarian State University |
| Citations | 4 |
Abstract
Section titled āAbstractāThe simulation of the temperature field in the diamond-polymer matrix system was conducted. The influence of the matrixās thermal conductivity on the temperature field was explored. Ways of reducing the thermal load on the tool were suggested.