Experimental realization of an absolute single-photon source based on a single nitrogen vacancy center in a nanodiamond
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2017-01-04 |
| Journal | Optica |
| Authors | Beatrice Rodiek, Marco López, Helmuth Hofer, G. Porrovecchio, Marek Šmíd |
| Institutions | Max Planck Institute for the Science of Light, Saarland University |
| Citations | 81 |
| Analysis | Full AI Review Included |
Executive Summary
Section titled “Executive Summary”- Objective: Experimental realization and absolute radiometric calibration of a single-photon source based on a single Nitrogen-Vacancy (NV) center in a nanodiamond, traceable to national metrology standards.
- Material Platform: Single NV center embedded in a commercial nanodiamond (Microdiamond AG, GAF 0.15), median size ~75 nm, dispersed on a 0.17 mm borosilicate cover glass.
- Excitation Scheme: Continuous-wave (CW) green laser at 532 nm through a high-NA oil-immersion confocal microscope (100×, NA 1.45); emission collected across 550-750 nm with multi-stage filtering.
- Calibration Chain: Photon flux measured via a low-noise silicon photodiode (LOFD) traceable to a cryogenic radiometer; spectral distribution independently characterized with a calibrated spectroradiometer.
- Key Performance Metrics: Adjustable radiant flux from ~55 fW (190,000 photons/s) to ~75 fW (260,000 photons/s); single-photon purity confirmed with g2(0) values between 0.10 and 0.23 across excitation powers up to 1.05 mW.
- Significance: First absolute calibration of a solid-state single-photon emitter through an unbroken traceability chain, enabling detector efficiency calibration and low-photon-flux metrology.
- Future Outlook: Pathway to deterministic sources through engineered dielectric or metallo-dielectric antenna structures and higher-purity diamond material to suppress background emission.
Technical Specifications
Section titled “Technical Specifications”| Parameter | Value | Unit | Context |
|---|---|---|---|
| Center Type | Nitrogen-Vacancy (NV-) | — | Active color center in nanodiamond |
| Host Material | GAF 0.15 nanodiamond | — | Commercial CVD-grown diamond powder |
| Nanodiamond Median Size | ~75 | nm | Per dimension |
| Substrate | Borosilicate microscope cover glass, 0.17 | mm | Spin-coated with nanodiamonds |
| Excitation Wavelength | 532 | nm | CW Laser Quantum Ventus |
| Excitation Power Range | Up to 1.05 (tested), ~1.25 (saturation) | mW | Delivered to nanodiamond |
| Saturation Power (Psat) | ~100 | µW | From three-level fit |
| Emission Spectral Range | 550 - 750 | nm | NV zero-phonon line at 637 nm |
| Detection Path | 550 nm long-pass; 750 & 800 nm short-pass | — | Multi-stage filtration |
| Detection Aperture | Single-mode fiber, 9 µm core | — | Confocal pinhole |
| Objective | 100×, NA 1.45 oil immersion | — | Nikon CFI Plan Apochromat Lambda |
| Excitation Spot | ~300-400 | nm | Elliptical, diffraction-limited |
| Radiant Flux (lowest) | ~55 | fW | At ~275 µW excitation |
| Radiant Flux (saturation) | ~75 | fW | At ~1.25 mW excitation |
| Photon Flux (lowest) | ~190,000 | photons/s | Corresponding to 55 fW |
| Photon Flux (saturation) | ~260,000 | photons/s | Corresponding to 75 fW |
| Saturation Photon Flux (Nsat) | ~240,000 | photons/s | Background-corrected |
| Single-Photon Purity g2(0) | 0.10 - 0.23 | — | Increases with excitation power |
| Calibration Detector | Hamamatsu S1227-33BQ Si photodiode (LOFD) | — | CMI-built switched integrator |
| Active Area of LOFD | 2.4 × 2.4 | mm | Free-space detection mode |
| Spectroradiometer | Horiba Jobin Yvon iHR 320 + CCD | — | Wavelength-resolved SPD |
| HBT Setup | 50:50 fiber splitter + 2× SPCM-AQRH-13-FC | — | TCSPC: PicoQuant PicoHarp 300 |
| Operating Temperature | Room temperature (~293 | K) | No cryogenic cooling required |
Key Methodologies
Section titled “Key Methodologies”- Sample Preparation
- Spin-coat NV-doped nanodiamond powder (GAF 0.15, ~75 nm median size) onto a 0.17 mm thick cover glass.
- Select a single nanodiamond containing exactly one NV center via confocal fluorescence scanning.
- Confocal Excitation & Collection
- Excite with a CW 532 nm laser through a laser line filter (LL01532-125) and dichroic beam splitter (FF560Di01).
- Focus with a 100×, NA 1.45 oil-immersion objective (Zeiss Immersol 518F immersion oil).
- Position via a piezo-electric translation stage (P563.3CD) for individual nanodiamond addressing.
- Spectral Filtering
- Notch filter (NF533, 17 nm bandwidth) plus dual short-pass filters (FES0750, FES0800) and a 550 nm long-pass filter (FEL0550).
- Confine detection with a 9 µm single-mode fiber serving as the spatial aperture.
- Radiometric Calibration
- Measure absolute radiant flux using the LOFD (switched integrator + Si photodiode), traceable to a cryogenic radiometer primary standard.
- Transition between fiber-coupled and free-space detection via matched 10×, NA 0.25 objectives.
- Spectral Characterization
- Acquire relative spectral power distribution Srel(λ) with a calibrated spectroradiometer (iHR 320 + CCD).
- Combine with LOFD output Uout and spectral responsivity sdet(λ) to compute absolute spectral photon flux Nph,λ(λ).
- Purity Verification
- Record second-order correlation function g2(τ) via HBT interferometer.
- Fit to a three-level rate-equation model to extract g2(0) and estimate background contribution factor m (27.6 µW−1·s−1).
- Saturation Modeling
- Fit experimental radiant flux vs. excitation power to determine Nsat ≈ 240,000 s−1 and Psat ≈ 100 µW.
- Subtract linear background term to isolate true NV-center photon flux.
6CCVD Solutions & Capabilities
Section titled “6CCVD Solutions & Capabilities”The research detailed above hinges on a defect-engineered fluorescent nanodiamond — a domain where MPCVD-grown diamond is the gold standard. 6CCVD is positioned to support any lab working on color-center photonics, single-photon metrology, or related quantum-radiometry projects by providing precisely controlled diamond substrates and active nanodiamonds.
Applicable Materials
Section titled “Applicable Materials”- Optical Grade Single Crystal Diamond (SCD): The absence of grain boundaries in SCD is critical to preserving long spin coherence and narrow inhomogeneous broadening of NV centers. For applications where a buried or implanted NV center is desired — a logical next step versus surface-bound nanodiamonds — 6CCVD supplies ultra-low nitrogen SCD with Ra < 1 nm polish, available in custom thicknesses from 0.1 µm to 500 µm.
- Polycrystalline Diamond (PCD): When studying ensemble behavior or fabricating larger-area substrates, optical-grade PCD wafers up to 125 mm provide a robust, scalable host. PCD is also a strong candidate for next-generation (metal-)dielectric antenna structures proposed by the authors for boosting collection efficiency.
- Heavy Boron-Doped PCD (BDD): For integration with plasmonic or metallo-dielectric antenna structures — flagged by the paper as a route to higher photon flux rates — 6CCVD’s conductive BDD can serve simultaneously as an active host and an electrical contact layer.
- CVD Nanodiamond Powder: 6CCVD can supply fractionated nanodiamond powders with controlled size distributions (down to sub-50 nm), suitable for spin-coating protocols identical to the one used in this work.
Customization Potential
Section titled “Customization Potential”- Dimensional Tailoring: The authors use ~75 nm particles on a 0.17 mm glass substrate. 6CCVD can deliver diamond in any geometry — freestanding membranes, thin films (down to 0.1 µm), or thick substrates (up to 10 mm) — and can laser-cut to user-defined footprints for hybrid integration.
- Surface Engineering for Photon Collection: To replicate or exceed the optical interface used here, 6CCVD offers Ra < 1 nm SCD polish and Ra < 5 nm PCD polish, minimizing scattering losses that contribute to the background emission the authors identify as a limiting factor.
- Custom Metalization for Hybrid Devices: For teams building the proposed antenna-coupled single-photon sources, 6CCVD provides in-house Ti, Pt, Pd, Au, W, and Cu metalization with photolithography-grade patterning. A Ti/Au stack, for instance, enables dipole-antenna geometries directly on the diamond surface.
- Traceable, Reproducible Material: Because every 6CCVD substrate ships with documented growth and post-processing parameters, batches are reproducible — a prerequisite when comparing radiometric measurements across labs.
Engineering Support
Section titled “Engineering Support”- PhD-Level Consultation: 6CCVD’s in-house PhD team routinely advises on color-center implantation, diamond-polymer hybrid integration, and surface functionalization for spin-coating protocols. Whether the application is single-photon metrology, quantum key distribution, or detector calibration, our engineers can help select the correct diamond grade, dopant concentration, and finishing recipe.
- Color-Center-Specific Recommendations: For projects targeting the Si-vacancy (SiV) emitters mentioned in the paper’s outlook — preferred for their narrow room-temperature linewidth — 6CCVD can deliver SCD substrates optimized for Si-ion implantation and high-temperature annealing recipes.
Call to Action
Section titled “Call to Action”For custom specifications, tailored doping profiles, or a confidential material consultation on your single-photon or quantum-radiometry program, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract
We report on the experimental realization of an absolute single-photon source based on a single nitrogen vacancy (NV) center in a nanodiamond at room temperature and on the calculation of its absolute spectral photon flux from experimental data. The single-photon source was calibrated with respect to its photon flux and its spectral photon rate density. The photon flux was measured with a low-noise silicon photodiode traceable to the primary standard for optical flux, taking into account the absolute spectral power distribution using a calibrated spectroradiometer. The optical radiant flux is adjustable from 55 fW, which is almost the lowest detection limit for the silicon photodiode, and 75 fW, which is the saturation power of the NV center. These fluxes correspond to total photon flux rates between 190,000 photons per second and 260,000 photons per second, respectively. The single-photon emission purity is indicated by a g((2))(0) value, which is between 0.10 and 0.23, depending on the excitation power. To our knowledge, this is the first single-photon source absolutely calibrated with respect to its absolute optical radiant flux and spectral power distribution, traceable to the corresponding national standards via an unbroken traceability chain. The prospects for its application, e.g., for the detection efficiency calibration of single-photon detectors as well as for use as a standard photon source in the low photon flux regime, are promising. (C) 2017 Optical Society of America