Magnetometry via spin-mechanical coupling in levitated optomechanics
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2017-01-01 |
| Authors | Pardeep Kumar, Mishkat Bhattacharya |
Abstract
Section titled āAbstractāWe analyze magnetometry using an optically levitated nanodiamond. We consider a configuration where a magnetic field gradient couples the mechanical oscillation of the diamond with its spin degree of freedom provided by a Nitrogen vacancy center. First, we investigate measurement of the position spectrum of the mechanical oscillator. We find that conditions of ultrahigh vacuum and feedback cooling allow a magnetic field gradient sensitivity of 1 $μ$Tm$^{-1}$/$\sqrt{\mbox{Hz}}$. At high pressure and room temperature, this sensitivity degrades and can attain a value of the order of 100 $m$Tm$^{-1}$/$\sqrt{\mbox{Hz}}$. Subsequently, we characterize the magnetic field gradient sensitivity obtainable by maneuvering the spin degrees of freedom using Ramsey interferometry. We find that this technique can offer photon-shot noise and spin-projection noise limited magnetic field gradient sensitivity of 100 $μ$Tm$^{-1}$/$\sqrt{\mbox{Hz}}$. We conclude that this hybrid levitated nanomechanical magnetometer provides a favorable and versatile platform for sensing applications.