The first quaternary diamond-like semiconductor with 10-membered LiS4rings exhibiting excellent nonlinear optical performances
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2017-01-01 |
| Journal | Chemical Communications |
| Authors | Kui Wu, Zhihua Yang, Shilie Pan |
| Institutions | Xinjiang Technical Institute of Physics & Chemistry |
| Citations | 100 |
Abstract
Section titled āAbstractāNew DLS-Li<sub>4</sub>HgGe<sub>2</sub>S<sub>7</sub>with novel 10-MR LiS<sub>4</sub>rings and excellent performances(concurrently large SHG coefficient and impressive LDT) is reported.