Diagnostics of service performance of diamond powders and diamond powder-based composite materials

MetadataDetails
Publication Date2017-06-30
JournalGornyi Zhurnal
AuthorsМ. Н. Сафонова, А. А. Федотов, A. S. Syromyatnikova
InstitutionsDiamant (Germany)

The number of particles per carat is a useful parameter which depends on the particle size distribution of a diamond batch.It is shown, that a two-dimensional image analysis can be used as an alternative method to the physical counting and weighing process for determining the particles per carat value.Theoretical reasons for measuring errors are discussed along with experimental results.In case of blocky saw grit diamond a factor of 1.2 can be applied to the image processing results in order to meet the physically counted values.