Growth of three-dimensional diamond mosaics by microwave plasma-assisted chemical vapor deposition

MetadataDetails
Publication Date2017-11-29
JournalCrystEngComm
AuthorsGuoyang Shu, Bing Dai, Victor Ralchenko, A. P. Bolshakov, А.А. Khomich
InstitutionsNational Research Nuclear University MEPhI, Prokhorov General Physics Institute
Citations14

Growth of novel 3D diamond mosaic structures by MPCVD was realized, clearing the way for complex diamond shapes.