A method of measuring micro-displacement based on spin magnetic resonance effect of diamond color center
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2018-01-01 |
| Journal | Acta Physica Sinica |
| Authors | Lei Wang, Guo Hao, Yulei Chen, Wu Da-Jin, Zhao Rui |
| Citations | 8 |
| Analysis | Full AI Review Included |
Executive Summary
Section titled “Executive Summary”- Core Innovation: Introduces a novel micro-displacement measurement method utilizing the electron spin magnetic resonance (ESR) effect of nitrogen-vacancy (NV) color centers in single crystal diamond (SCD), bypassing the hysteresis and non-linearity limitations inherent to traditional piezoelectric ceramic sensors.
- Theoretical Mechanism: Establishes a correlation model linking the Zeeman splitting of the NV center’s ground state to a magnetic gradient field generated by a cylindrical NdFeB permanent magnet, where position dictates magnetic field strength.
- Key Achievement: Demonstrates a measurement sensitivity of 16.67 V/mm with a detection resolution of 60 nm.
- Experimental Validation: The optically detected magnetic resonance (ODMR) spectrum yielded a linear relationship of 2.79 MHz/Gauss between Zeeman splitting and magnetic field intensity.
- Magnetic Field Mapping: A high-precision Gauss meter mapped a linear magnetic gradient region of −7.77 Gauss/mm along the magnet’s central axis within a 4-7 mm distance range.
- Future Scaling: Theoretical analysis indicates that reducing the distance between the NV diamond sensor and the magnet surface (down to micrometer scale) can push the resolution beyond the current limits, achieving sub-nanometer precision.
- Application Horizon: Provides a robust, cost-effective, and highly precise research pathway for next-generation atomic force microscopy (AFM) and scanning probe microscopy (SPM) systems.
Technical Specifications
Section titled “Technical Specifications”| Parameter | Value | Unit | Context |
|---|---|---|---|
| Diamond Material Type | Type Ib | Single Crystal Diamond (SCD) | Substrate for NV center formation |
| Diamond Dimensions | 4.5 x 4.5 x 0.5 | mm | Commercial Element 6 sample |
| Crystal Orientation | (100) | Crystallographic Plane | Polished surface |
| NV Axis Alignment | [111] | Crystallographic Direction | Parallel to displacement axis |
| Zero-Field Splitting (D) | 2.87 | GHz | Energy gap between m_s = 0 and m_s = ±1 |
| ESR Resonance Frequency | 3000.56 | MHz | Lock-in demodulation target frequency |
| Spectral Linewidth (FWHM) | 15.24 | MHz | Right-side resonance dip of normalized ESR curve |
| Zeeman Splitting Sensitivity | 2.79 | MHz/Gauss | Linear correlation coefficient: 0.99787 |
| Measurement Sensitivity | 16.67 | V/mm | System voltage output per millimeter of displacement |
| Displacement Resolution | 60 | nm | Calculated from 1 mV system noise standard deviation |
| Measurement Range | ±0.35 | mm | Total span within the linear magnetic gradient |
| Magnet Material | N35 Sintered NdFeB | Permanent Magnet | Cylindrical geometry |
| Magnet Dimensions (r x h) | 8 x 10-3 x 1 x 10-3 | m (radius x height) | Uniformly magnetized along axis |
| Magnetization Strength (M) | 0.1229 | T | Axial magnetization |
| Magnetic Gradient (dH/dz) | −7.77 | Gauss/mm | Measured linear region (4-7 mm from surface) |
| Linear Correlation (Field) | 0.99725 | R2 | Gauss meter field mapping |
| Excitation Laser Wavelength | 532 | nm | Green laser for NV polarization |
| Microwave Modulation Frequency | 25.8 | kHz | External signal source modulation |
| Microwave Modulation Amplitude | 1.5 | V | Signal modulation depth |
| Lock-in Demodulation Slope (α) | 0.74 | V/MHz | Output voltage slope across FWHM |
| Magnetic Shielding Residual Field | < 0.1 | nT | CPBT-W7 magnetic shielding system |
Key Methodologies
Section titled “Key Methodologies”- Material Preparation: Utilize a commercial Type Ib SCD with specific crystallographic alignment; the polished (100) surface and [111] NV axis orientation are critical for uniform ESR response.
- Magnetic Field Profiling: Use a high-precision Model 931 Gauss meter to map the z-axis magnetic intensity of a cylindrical NdFeB magnet.
- Linear Region Identification: Identify and isolate the 4-7 mm region from the magnet surface where the magnetic gradient exhibits strict linearity (R2 > 0.99).
- Optically Detected Magnetic Resonance (ODMR) Setup: Assemble a confocal microscopy setup featuring a 532 nm green laser, a dichroic mirror (380-550 nm reflection, 584-700 nm transmission), and a 550-750 nm bandpass filter.
- Microwave Delivery: Apply a modulated microwave signal (25.8 kHz, 1.5 V) via a microwave antenna directly to the diamond sample to induce electron spin transitions.
- Fluorescence Detection: Collect the modulated ESR fluorescence via a photodetector, splitting the signal for direct observation and lock-in amplification.
- Displacement Control: Mount the permanent magnet on a high-precision displacement stage (0.01 mm minimum resolution) and adjust the relative distance in increments (0.1 mm to 0.5 mm).
- Signal Demodulation: Employ a lock-in amplifier to extract the Zeeman splitting signal, converting the resonance frequency shift into a measurable voltage output (V).
- Environmental Isolation: Enclose the entire test setup within a high-performance magnetic shielding system to suppress geomagnetic and ambient RF interference.
6CCVD Solutions & Capabilities
Section titled “6CCVD Solutions & Capabilities”-
Applicable Materials: To replicate or extend this quantum sensing research, an Optical Grade Type Ib Single Crystal Diamond (SCD) is required. 6CCVD provides high-purity SCD substrates grown via MPCVD, featuring precisely controlled [111] crystallographic orientations essential for maximizing NV center yield and ensuring uniform Zeeman splitting responses.
-
Customization Potential: The paper utilized a 4.5 mm x 4.5 mm x 0.5 mm diamond plate. 6CCVD specializes in custom dimensions, capable of manufacturing SCD plates and wafers tailored to specific geometries required for unique confocal setups or integrated scanning probes. Furthermore, if your experimental design requires integrated microwave antennas or specific bonding pads, our in-house custom metalization services (Ti/Pt/Au, W, etc.) can deposit patterned electrodes directly onto the diamond surface.
-
Enhanced NV Density: For researchers looking to push sensitivity limits toward the sub-nanometer scale proposed by the authors, 6CCVD offers custom-engineered diamond substrates optimized for high-density NV center creation via precise nitrogen doping during the MPCVD growth process.
-
Engineering Support: The transition from a 60 nm resolution to sub-nanometer precision requires meticulous control over material defects, surface roughness (we offer SCD polishing down to Ra < 1 nm), and magnetic impurity levels. Our in-house PhD engineering team can provide direct material consultation to help optimize your diamond sensor for advanced AFM, SPM, or precision metrology projects.
-
Call to Action: For custom specifications, bespoke material consultation, or to discuss your precision sensing requirements, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract
As one of the excellent piezoelectric materials, piezoelectric ceramic has been widely used to develop a highly precise displacement measurement system, which is the key part of the scanning probe system of the high-precision measuring instrument.Based on the high-precision scanning probe system, the micro/nano structures can be easily and accurately detected by the instrument system.However, due to the limitations caused by the character of hysteresis and nonlinearity, it is difficult to further improve the precision of highly precise displacement measurement system.In this work, we present a novel method to develop the highly precise displacement measurement system based on the quantum spin effect.The nitrogen vacancy (NV) color center of single crystal diamond as a sensitive element senses the change of the micro-displacement.Based on the electron spin magnetic resonance effect of diamond nitrogen vacancy color center, the variation of the magnetic field generated from the magnetic steel can be detected with high precision by the electron spin.The relative relation between the displacement and the magnetic gradient field can be used to establish the correlation model between the displacement and the electron spin resonance peak.In the experiment, a corresponding micro-displacement measurement system is established based on the cylindrical permanent magnet, according to the correlation model between the electron spin resonance effect and micro-displacement.The linear region of magnetic field gradient is designed to detect the micro-displacement.Firstly, the intensity distribution of magnetic field gradient is measured by the gauss meter.As the measurement results show, the gradient value is -7.77 Gauss/mm along the core axis of cylindrical permanent magnet, and the intensity of magnetic field gradient distribution region is linear in the millimeter range.Meanwhile, the electron spin magnetic resonance peak of diamond nitrogen vacancy color center is achieved by the optically detected magnetic resonance technology.The electron spin magnetic resonance peak is approximately 2.79 MHz/Gauss in the magnetic field achieved by the fluorescence spectrum of diamond nitrogen vacancy color center, attributed to the relation model between Zeeman splitting effect and magnetic field. In the experiment, the electron spin magnetic resonance signal of diamond nitrogen vacancy color center is lockedin by the demodulation method to achieve the change of micro-displacement.As the results show, the sensitivity is about 16.67 V/mm at the corresponding demodulation frequency of 3000.56 MHz.By the calculation, the resolution of micro-displacement measurement system is about 60 nm based on our method.It proves out a high precision and well reliability method to detect the micro-displacement.By the further theoretical calculation, based on the electron spin effect, the detection resolution of our method can be enhanced up to sub-nanometer scale by reducing the distance between the NV color center and the magnet.It presents a new research direction and field for the micro-displacement detection system.