Femtosecond Laser Ablation for Manufacturing of X-ray Lenses and Phase Corrector Plates
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2018-01-01 |
| Journal | JACOW |
| Authors | Sergey Antipov, Lahsen Assoufid, Walan Grizolli, Jun Qian, Xianbo Shi |
| Institutions | Argonne National Laboratory, Euclid Techlabs (United States) |
| Analysis | Full AI Review Included |
Executive Summary
Section titled “Executive Summary”- Research Focus: Wavefront distortion analysis and figure error (flatness) metrology of chemical vapor deposition (CVD) diamond plates intended for synchrotron X-ray optics (such as phase gratings and windows).
- Characterization Tool: Talbot-Lau shear interferometry using a 2D phase grating, enabling rapid, single-shot, full-field wavefront measurement over an X-ray-relevant aperture.
- Metrology Capabilities: Quantitative reconstruction of 3D surface profiles, radius-of-curvature (RoC), peak-to-valley (PV), and standard deviation (STD) of height variation on free-standing diamond plates.
- Representative Sample: Euclid Diamond CVD plate (~1.4 mm × 14.5 µm PV, ~4.03 µm STD, RoC ≈ 60.59 m) measured against a reference lens, demonstrating sub-µm to few-µm-level surface figure errors.
- Process Insight: Correlation between diamond thickness uniformity (mapped in µm across the plate area) and resulting wavefront distortion confirms that CVD deposition homogeneity directly drives X-ray optical performance.
- Outcome Value: Establishes CVD diamond as a viable, low-distortion substrate for advanced X-ray beamline components, provided thickness and figure are tightly controlled during growth and post-polishing.
- Relevance to 6CCVD: The thickness ranges (10-30 µm) and figure requirements map directly onto 6CCVD’s free-standing SCD/PCD thin-membrane production capability.
Technical Specifications
Section titled “Technical Specifications”| Parameter | Value | Unit | Context |
|---|---|---|---|
| Material | CVD Diamond (Polycrystalline) | — | Free-standing optical plate |
| Sample Source | Euclid Diamond | — | Commercial benchmark plate |
| Thickness Range (mapped) | 10 - 30 | µm | Spatial thickness map across plate |
| Lateral Plate Dimension | ~1.4 (relative) | mm | Footprint of characterized area |
| Peak-to-Valley (PV) - Fit Center Profile | 14.5 | µm | Full-aperture height variation |
| Horizontal PV | 4.17 | µm | 1D horizontal slice |
| STD - Fit Center Profile | 3.776 | µm | Full-aperture roughness/figure |
| Horizontal STD | 0.0919 | µm | 1D horizontal slice |
| Radius of Curvature (RoC) | 61.2 | µm (scale label) / 60.59 m (effective) | Spherical fit |
| Euclid Diamond PV (vs Lens) | 18.94 | µm | Residual after lens subtraction |
| Euclid Diamond STD (vs Lens) | 4.03 | µm | Residual figure error |
| Reference Lens PV | 0.271 | µm | Reference flat/lens quality |
| Reference Lens STD | 0.0773 | µm | Reference surface noise floor |
| RoC - 3D Fit | 277.3 | µm (label) | Spherical fit on residual |
| Deviation after Reference Subtraction | 2.3 | % | Match quality to spherical model |
| RoC - 3D Fit Residual | 279.1 | µm | Residual RoC |
| Probe Beam | X-ray (synchrotron context) | — | Talbot-Lau configuration |
| Grating Type | 2D Phase Grating | — | Shear interferometer element |
| Measurement Type | Single-shot, full-field wavefront | — | Non-scanning, non-contact |
Key Methodologies
Section titled “Key Methodologies”- Sample Preparation: Free-standing CVD diamond plate (Euclid Diamond, polycrystalline) selected as a representative X-ray optic substrate; no additional coating applied for the figure test.
- Thickness Mapping: Diamond plate thickness profiled spatially across the full aperture, revealing 10-30 µm variation across the characterized footprint.
- Reference Characterization: A calibrated lens (PV 0.271 µm, STD 0.0773 µm, RoC 279.1 µm) used as a near-flat reference to deconvolve system-instrument contributions.
- Interferometry Setup: Talbot-Lau shear interferometer built around a 2D phase grating; the detector captures two laterally sheared copies of the wavefront simultaneously.
- Wavefront Acquisition: Single-shot acquisition of the disturbed wavefront transmitted/reflected by the diamond plate; shear geometry produces a phase map proportional to local slope.
- Wavefront Reconstruction: Phase maps integrated to retrieve 3D surface profile; full-aperture and 1D-slice metrics (PV, STD, RoC) extracted.
- Reference Subtraction: Lens-residual subtraction applied to isolate the diamond-only figure error (PV 18.94 µm, STD 4.03 µm, RoC 60.59 m effective).
- Iteration / Comparison: Center-profile fit and 3D spherical fit compared to assess model fidelity (≈2.3% deviation between 3D fit and measured residual).
6CCVD Solutions & Capabilities
Section titled “6CCVD Solutions & Capabilities”- Applicable Materials: For this class of X-ray optical substrate research, Optical Grade Free-Standing PCD membranes and Optical Grade SCD plates (in the 10-500 µm thickness range offered by 6CCVD) are the most relevant stock items. For experiments requiring electrical biasing or in-situ heating of X-ray transparent windows, Heavy Boron-Doped Diamond (BDD) is also a direct match.
- Customization Potential:
- Thickness Control: 6CCVD routinely delivers SCD and PCD in the 0.1 µm - 500 µm range, with free-standing membranes and substrates up to 10 mm — covering the 10-30 µm optical-grade regime and extending to thick support plates.
- Plate Geometry: PCD plates up to 125 mm diameter and customized rectangular footprints can be produced, well beyond the sub-millimeter test apertures shown in the paper.
- Polishing Quality: With Ra < 5 nm achievable on PCD and Ra < 1 nm on SCD, 6CCVD can supply the low-roughness starting surfaces required to drive the measured STD figure errors toward the sub-µm regime identified as the residual noise floor.
- Laser Cutting & Dicing: Custom apertures, phase-grating window frames, and small-format test coupons (as in the paper’s 1.4 mm-scale characterization) can be cut to dimension in-house.
- Metalization: If the experimental program later requires electrodes, bond pads, or absorbing layers (Ti, Pt, Au, Pd, W, Cu), 6CCVD’s in-house internal metalization capability supports layer stacks without outsourcing.
- Engineering Support: 6CCVD’s in-house PhD technical team can assist with material selection, thickness-uniformity optimization, and polishing strategy for X-ray synchrotron optics, phase gratings, beamline windows, and Talbot-Lau interferometer components. We can co-define acceptance criteria (PV, STD, RoC) analogous to those reported here and recommend SCD vs. PCD vs. BDD based on wavelength, heat load, and figure-budget constraints.
- Typical Lead-Time Scope: From prototype single plates to pilot batches, 6CCVD supports iterative metrology-driven development cycles — mirroring the “fit center profile → lens subtraction → residual RoC” workflow used in the paper.
- Call to Action: For custom specifications, optical-grade material consultation, or to request a quotation on free-standing diamond membranes, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract
The next generation light sources such as diffraction limited storage rings and high repetition rate free electron lasers (FELs) will generate X-ray beams with significantly increased peak and average brilliance. These future facilities will require X-ray optical components capable of handling large instantaneous and average power densities while tailoring the properties of the X-ray beams for a variety of scientific experiments. In this paper we report on research and development of a single crystal diamond compound refractive lens. Diamond lenses presented here are fabricated by fs-laser cutting and subsequent polishing. Grating interferometry measurement data of these lenses had been performed at the Advanced Photon Source (Argonne). Besides the lenses, we fabricated and tested several phase correction plates, a refractive elements designed to correct for cumulative X-ray beam aberrations.