Prospects of Spin Gyroscopes Based on Nitrogen-Vacancy Centers in Diamond
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2018-01-01 |
| Journal | Latin America Optics and Photonics Conference |
| Authors | Andrey Jarmola, Dmitry Budker, Sami Hawasli, A. Glen Birdwell, Tony Ivanov |
| Institutions | University of California, Berkeley, DEVCOM Army Research Laboratory |
Abstract
Section titled āAbstractāWe are developing a solid-state gyroscope based on ensembles of nitrogen-vacancy centers in diamond. Rotation of the nitrogen-vacancy symmetry axis will induce Berry phase shifts in the electronic ground state 14N hyperfine sublevels and can be measured with a Ramsey technique.