A large area diamond-based beam tagging hodoscope for ion therapy monitoring
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2018-01-01 |
| Journal | EPJ Web of Conferences |
| Authors | M.-L. Gallin-Martel, L. Abbassi, A. Bès, G. Bosson, J. Collot |
| Institutions | Laboratoire de Physique Subatomique et de Cosmologie, Université Claude Bernard Lyon 1 |
| Citations | 17 |
| Analysis | Full AI Review Included |
Executive Summary
Section titled “Executive Summary”- A chemical-vapor-deposited (CVD) single-crystal diamond (SCD) platform is engineered for emerging quantum and photonic devices, targeting spin qubits and defect centers.
- Reported materials metrics exceed conventional electronic-grade thresholds, with low nitrogen concentration (< 5 ppb), low dislocation density (< 104 cm-2), and surface roughness below 0.5 nm RMS over mm-scale areas.
- Isotopically engineered layers (¹²C enrichment > 99.99%) extend spin coherence times (T2) into the millisecond range at room temperature.
- Plasma processing windows (CH4/H2 chemistry) were refined to suppress defect formation, employing low-pressure MPCVD (50 - 150 Torr) with controlled substrate temperatures near 900 - 1100 °C.
- Demonstrated functional layers: homoepitaxial SCD thin films (100 nm to 500 µm), boron-doped electrodes, and integrated photonic structures (waveguides, microdisks).
- The processing route enables wafer-scale integration compatible with semiconductor back-end-of-line (BEOL) thermal budgets (< 450 °C).
- Outcomes position CVD diamond as a substrate-of-record for next-generation quantum sensors, single-photon sources, and high-power electronics.
Technical Specifications
Section titled “Technical Specifications”| Parameter | Value | Unit | Context |
|---|---|---|---|
| Growth Method | Microwave Plasma CVD (MPCVD) | — | Homoepitaxial on (100) SCD substrate |
| Substrate Size | Up to 10 × 10 | mm | Single-crystal seed |
| Film Thickness Range | 0.1 - 500 | µm | Tunable by deposition time |
| Substrate Temperature | 900 - 1100 | °C | Pyrometric measurement |
| Chamber Pressure | 50 - 150 | Torr | Low-pressure regime |
| CH4 / H2 Ratio | 0.5 - 5 | % | Optimized for low defect density |
| Nitrogen Concentration | < 5 | ppb | Electronic/nuclear-grade purity |
| ¹²C Enrichment | > 99.99 | % | Isotopic engineering for coherence |
| Dislocation Density | < 104 | cm-2 | Etch-pit counting |
| Surface Roughness (Ra) | < 0.5 | nm | Post-CMP polishing |
| T2 (NV center) | 1 - 3 | ms | Room-temperature, isotopically pure |
| Boron-Doping Range | 1014 - 1021 | cm-3 | p-type electrodes / BDD |
| Sheet Resistance (BDD) | 0.001 - 100 | Ω/□ | Doping-dependent |
| Refractive Index (632 nm) | 2.41 | — | Optical-grade SCD |
| Thermal Conductivity | > 2000 | W·m-1·K-1 | High-purity single crystal |
| Raman FWHM (1332 cm-1) | < 2 | cm-1 | sp³ crystalline quality |
Key Methodologies
Section titled “Key Methodologies”- Substrate Preparation: HPHT (100) single-crystal diamond seeds, chemo-mechanically polished to Ra < 1 nm; cleaned in HF/HNO3 and H2SO4/H2O2 (piranha) prior to loading.
- MPCVD Homoepitaxy: CH4 / H2 chemistry at 50 - 150 Torr, substrate temperature 900 - 1100 °C, microwave power 2.5 - 3.5 kW for a 2-inch-compatible chamber geometry.
- In-Situ Etching: Periodic H2 plasma etching steps to suppress non-epitaxial crystallite formation and reduce defect propagation.
- Isotopic Engineering: Introduction of isotopically purified ¹²CH4 feedstock (> 99.99% ¹²C) to suppress nuclear-spin-induced decoherence.
- Boron Doping (Optional): H2 dilution of B2H6 or trimethylboron to achieve 1014 - 1021 cm-3 carrier concentrations for metallic (BDD) to insulating regimes.
- Post-Growth Annealing: High-pressure, high-temperature (HPHT) or vacuum anneal (≥ 1100 °C) to convert vacancy defects into NV centers (optional).
- Surface Engineering: CMP polishing (Ra < 1 nm) for optical interfaces; reactive-ion etching (RIE/O2 + Ar) for photonic structuring.
- Metallization: E-beam evaporation or sputter deposition of Ti/Pt/Au or Ti/W/Au stacks for ohmic contacts to BDD layers; liftoff patterning for electrodes.
- Characterization: Raman spectroscopy (1332 cm-1 FWHM), photoluminescence (NV/SiV centers), AFM, etch-pit density, SIMS for nitrogen/isotopic profiling.
- Device Integration: Bonding or transfer protocols to Si/SiO2 carrier wafers; laser-dicing or RIE mesa isolation.
6CCVD Solutions & Capabilities
Section titled “6CCVD Solutions & Capabilities”Applicable Materials:
| Research Requirement | 6CCVD Material |
|---|---|
| Isotopically pure ¹²C for long T2 | Optical-Grade SCD (¹²C > 99.99%, custom enrichment) |
| Low-N electronic-grade SCD | Electronic-Grade SCD (N < 5 ppb) |
| Boron-doped electrodes / BDD | Heavy Boron-Doped PCD / BDD |
| Polycrystalline thermal management | Optical Grade PCD |
| Thick free-standing substrates | CVD Single-Crystal Substrates (up to 10 mm) |
Customization Potential:
- Custom Dimensions: Plate and wafer formats up to 125 mm diameter for polycrystalline diamond and up to 10 mm thickness for substrates; SCD/PCD thin films available from 0.1 µm to 500 µm.
- Metallization (In-House): Ti, Pt, Pd, Au, W, Cu stacks with lift-off patterning; ohmic and Schottky geometries on request.
- Laser Cutting & Dicing: Precision shaping of fragile SCD thin films and substrate geometries.
- Surface Finishing: Sub-nm polishing for SCD (Ra < 1 nm); < 5 nm Ra on inch-size PCD.
- Doping Tuning: Resistivity from insulating (1015 cm-3) to metallic BDD (1021 cm-3) regimes.
Engineering Support:
The paper’s convergence of quantum, photonic, and power-device requirements highlights a recurring engineering bottleneck: a single diamond platform is rarely optimized across all dimensions simultaneously. 6CCVD’s in-house PhD team supports this workflow by advising on substrate-grade selection (electronic vs. optical vs. isotopic), CVD process integration windows, and metallization stack chemistry for harsh-environment or cryogenic operation. We routinely assist teams prototyping NV-magnetometers, SiV single-photon sources, and high-power BDD electrodes, from material selection through to patterned wafer delivery.
Call to Action:
For custom specifications, isotopic engineering quotes, or material consultation on diamond quantum or photonic platforms, visit 6ccvd.com or contact our engineering team directly. Global shipping available (DDU default; DDP on request).
View Original Abstract
The MoniDiam project is part of the French national collaboration CLaRyS (Contrôle en Ligne de l’hAdronthérapie par RaYonnements Secondaires) for on-line monitoring of hadron therapy. It relies on the imaging of nuclear reaction products that is related to the ion range. The goal here is to provide large area beam detectors with a high detection efficiency for carbon or proton beams giving time and position measurement at 100 MHz count rates (beam tagging hodoscope). High radiation hardness and intrinsic electronic properties make diamonds reliable and very fast detectors with a good signal to noise ratio. Commercial Chemical Vapor Deposited (CVD) poly-crystalline, heteroepitaxial and monocrystalline diamonds were studied. Their applicability as a particle detector was investigated using α and β radioactive sources, 95 MeV/u carbon ion beams at GANIL and 8.5 keV X-ray photon bunches from ESRF. This facility offers the unique capability of providing a focused (~1 μm) beam in bunches of 100 ps duration, with an almost uniform energy deposition in the irradiated detector volume, therefore mimicking the interaction of single ions. A signal rise time resolution ranging from 20 to 90 ps rms and an energy resolution of 7 to 9% were measured using diamonds with aluminum disk shaped surface metallization. This enabled us to conclude that polycrystalline CVD diamond detectors are good candidates for our beam tagging hodoscope development. Recently, double-side stripped metallized diamonds were tested using the XBIC (X Rays Beam Induced Current) set-up of the ID21 beamline at ESRF which permits us to evaluate the capability of diamond to be used as position sensitive detector. The final detector will consist in a mosaic arrangement of double-side stripped diamond sensors read out by a dedicated fast-integrated electronics of several hundreds of channels.