Next-Generation, Super-Hard-to-Process Substrates and Their High-Efficiency Machining Process Technologies Used to Create Innovative Devices
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2018-03-01 |
| Journal | International Journal of Automation Technology |
| Authors | Toshiro Doi |
| Citations | 11 |
Abstract
Section titled āAbstractāSiC, GaN, and diamond are known as super-hard-to-process substrate for next-generation green devices. In this paper, we report on some breakthrough in developing highly efficient processing for such hard-to-process materials, for which we propose improvements in conventional processing, and innovative processing. As part of our project, we developed a ādilatancy padĀ®ā that can efficiently produce high-quality surfaces as well as a high-rigidity, high-speed and high-pressure processing machine. We also designed and prototyped āplasma fusion CMPĀ®,ā which is an innovative processing technology fusing CMP (Chemical Mechanical Polishing) with P-CVM (Plasma Chemical Vaporization Machining) to machine super-hard diamond substrates that are considered indispensable for future devices. Before the advent of āsingularitiesā by 2045, super-hard-to-process substrates and ultra-precision polishing technology will become more and more essential.