Band offset and electronic properties at semipolar plane AlN($1bar{1}01$)/diamond heterointerface
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2018-05-01 |
| Journal | Chinese Physics B |
| Authors | Kongping Wu, Wenfei Ma, Changxu Sun, Changzhao Chen, Liuyi Ling |
| Citations | 4 |
Abstract
Section titled āAbstractāTailoring the electronic states of the AlN/diamond interface is critical to the development of the next-generation semiconductor devices such as the deep-ultraviolet light-emitting diode, photodetector, and high-power high-frequency field-effect transistor. In this work, we investigate the electronic properties of the semipolar plane AlN()/diamond heterointerfaces by using the first-principles method with regard to different terminated planes of AlN and surface structures of diamond (100) plane. A large number of gap states exist at semi-polar plane AlN()/diamond heterointerface, which results from the N 2p and C 2s2p orbital states. Besides, the charge transfer at the interface strongly depends on the surface termination of diamond, on which hydrogen suppresses the charge exchange at the interface. The band alignments of semi-polar plane AlN()/diamond show a typical electronic character of the type-II staggered band configuration. The hydrogen-termination of diamond markedly increases the band offset with a maximum valence band offset of 2.0 eV and a conduction band offset of 1.3 eV for the semi-polar plane N-AlN()/hydrogenated diamond surface. The unique band alignment of this Type-II staggered system with the higher CBO and VBO of the semi-polar AlN/HC(100) heterostructure provides an avenue to the development of robust high-power high-frequency power devices.