Development of Diamond Tracking Detectors for High Luminosity Experiments at the LHC, HL-LHC and Beyond
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2018-05-27 |
| Journal | CERN Document Server (European Organization for Nuclear Research) |
| Authors | H. Kagan, W. Trischuk |
| Citations | 6 |
| Analysis | Full AI Review Included |
Executive Summary
Section titled “Executive Summary”- Goal: Development of radiation-tolerant polycrystalline Chemical Vapor Deposition (pCVD) diamond tracking detectors for the High Luminosity Large Hadron Collider (HL-LHC), targeting operation up to 1017 hadrons/cm2.
- Key Achievement: Verified that pCVD diamond detectors exhibit rate-independent signal pulse height up to 20 MHz/cm2 even after irradiation with 4 × 1015 n/cm2 — a critical breakthrough for high-luminosity environments.
- Innovation: Fabrication and successful testing of the first pCVD 3D pixel detector with 50 µm × 50 µm cells, achieving 99.2% MIP detection efficiency at a 1500 e threshold, with charge collection exceeding 75% of deposited charge.
- Application Scope: Planar pixel modules installed and operational in ATLAS (Diamond Beam Monitor) and CMS (BCM1F), with ongoing work on 3D pixel tracking for HL-LHC inner tracker upgrades.
- Material Milestone: As-grown 12 cm diameter pCVD wafers now routinely achieve >400 µm charge collection distance with 5% uniformity across the wafer, with thickness specifications of 500 µm ± 10 µm.
- 3D Electrode Fabrication: Laser-processed columns (2.5 µm diameter), with parallel development of plasma etching techniques for sub-5 µm diameter electrode holes.
- Long-term Vision: Transfer mature 3D diamond technology to industry, scale sensors to 10 cm2 active areas, and qualify devices for operation across LHC Runs 4 and 5 without replacement.
Technical Specifications
Section titled “Technical Specifications”| Parameter | Value | Unit | Context |
|---|---|---|---|
| Charge Collection Distance (as-grown) | > 400 | µm | 12 cm pCVD wafer production |
| Charge Collection Uniformity | 5 (target <2 by 2021) | % | Across 12 cm wafer |
| pCVD Wafer Diameter | 12 | cm | Production reactor output |
| Sample Thickness (typical) | 500 | µm | Standard detector grade |
| Sample Thickness (range) | 0.1 - 500 | µm | 6CCVD SCD/PCD capability match |
| Bias Voltage (standard operation) | ±1 to ±2 | V/µm | Equivalent to ±500 V to ±1000 V |
| Bias Voltage (ATLAS DBM) | 500 | V | Field = 1 V/µm |
| Leakage Current (pre-irradiation threshold) | < 10 | nA | After Sr-90 pumping |
| Beam-induced Current Test | 20 | nA | HV stability validation |
| 3D Pixel Cell Size | 50 × 50 (target 25 × 25) | µm | 3D pCVD pixel detector |
| 3D Column Diameter | 2.5 | µm | Laser-drilled electrodes |
| Plasma Etch Hole Diameter Target | < 5 | µm | Alternative fabrication route |
| Strip Pitch (strip modules) | 50 | µm | With 25 µm strip width |
| Strip Count per Module | 128 | channels | VA2.2 ASIC readout |
| ATLAS DBM Pixel Count | 26,880 | pixels | FE-I4 chip |
| ATLAS DBM Active Area | 16.8 × 20.0 | mm × mm | 250 µm × 50 µm pitch |
| ATLAS DBM Module Dimensions | 18 × 21 | mm × mm | 500 µm thick pCVD |
| Readout Noise (strip) | ~ 80 | e- | Common mode corrected |
| Readout Noise (pad/pixel) | ~ 550 | e- | 2 pF input capacitance |
| Front-end Peaking Time | ~ 6 | ns | Custom amplifier |
| Return-to-Baseline Time | ~ 16 | ns | Custom amplifier |
| Particle Flux Tested (rate studies) | 5 kHz to 20 | MHz/cm2 | π+ at PSI HIPA |
| MIP Detection Threshold (3D pixel) | 1500 | e- | CMS pixel electronics |
| 3D Pixel Hit Efficiency | 99.2 (planar Si: 99.7) | % | Un-irradiated, 67 kHz/cm2 |
| 3D Charge Collection | > 75 (target > 90) | % | Of deposited charge |
| Radiation Hardness (proven) | 2 × 1016 | p/cm2 | High-quality pCVD diamond |
| Radiation Hardness (program target) | 1017 | neq/cm2 | HL-LHC qualification |
| Damage Constant (800 MeV p) | 1.85 ± 0.13 | — | Normalized to 24 GeV p |
| Damage Constant (70 MeV p) | 2.5 ± 0.4 | — | Normalized to 24 GeV p |
| Damage Constant (25 MeV p) | 4.5 ± 0.6 | — | Normalized to 24 GeV p |
| Damage Constant (fast neutrons) | 4.5 ± 0.5 | — | Normalized to 24 GeV p |
| Surface Imperfection Target | < 1 | /cm2 | Voids and defects |
| Working Temperature | Cryogenic-capable | — | Dipole cryostat BLM |
| Front-end ASIC Technology | 65 nm CMOS | — | VLSI for HL-LHC BLM |
Key Methodologies
Section titled “Key Methodologies”- Beam Test Setup: Performed at PSI πM1 beamline with 260 MeV/c π+ at fluxes spanning 5 kHz/cm2 to 20 MHz/cm2, 19.8 ns bunch spacing.
- Telescope Reference Tracking: 100 µm × 150 µm CMS silicon pixel sensors with PSI46v2 readout chip for precise track reconstruction (~2 µm position resolution from 8-plane Si strip telescope).
- Readout Electronics: Custom-built amplifier (6 ns peaking time, 550 e- noise at 2 pF), DRS4 evaluation board digitizing at 2 GS/s.
- Sample Preparation: Hot acid cleaning → oxygen plasma etching → photolithographic lift-off metallization (50 µm pitch, 25 µm strip width) → Sr-90 “pumping” to fill intrinsic traps.
- Irradiation Facilities:
- 800 MeV protons at LANSCE (Los Alamos)
- 70 MeV protons at CYRIC (Tohoku University)
- Fast reactor neutrons (>100 keV) at JSI TRIGA reactor
- 24 GeV protons and 120 GeV/c hadrons at CERN SPS H6 beamline
- Radiation Damage Model: Linear dependence 1/λ = 1/λ0 + kφ, where λ is the mean free path and k is the damage constant extracted per sample.
- 3D Electrode Fabrication: Laser column drilling (current method) and plasma etching of sub-5 µm holes followed by conductive fill (development track).
- 3D Cell Geometry: Bias electrodes at 4 corners of cubic cells, readout electrodes at cell center; 3 × 2 ganging for CMS readout chip compatibility.
- Characterization Suite: Plasma processing → crossed-polarizer visible inspection for stress/defects → IV/CV curves with and without beam-induced current → charge collection and MFP measurements at 10 Hz to 10 kHz.
- Data Analysis Cuts: Removal of heavily ionizing saturated waveforms, calibration triggers, wrong-bucket triggers, and out-of-fiducial tracks; systematics estimated from data scatter below 80 kHz/cm2.
6CCVD Solutions & Capabilities
Section titled “6CCVD Solutions & Capabilities”Applicable Materials
Section titled “Applicable Materials”- Electronic Grade Polycrystalline Diamond (PCD): Directly applicable for replicating and extending the RD42 results. 6CCVD PCD is available in thicknesses from 0.1 µm to 500 µm and substrates up to 10 mm, matching the 500 µm detector-grade material requirements with high charge collection distance.
- Single Crystal Diamond (SCD): Suitable for reference samples and the parallel scCVD track in the radiation damage studies. 6CCVD SCD supports thicknesses 0.1 µm to 500 µm with Ra < 1 nm polishing.
- Large-Format PCD Wafers: 6CCVD provides plates/wafers up to 125 mm, aligned with the 12 cm pCVD wafer scale referenced in the paper.
- Laser-Cut 3D Cell Geometries: 6CCVD offers laser cutting and structuring services for the 50 µm × 50 µm and 25 µm × 25 µm cell patterns with 2.5 µm diameter column electrodes.
Customization Potential
Section titled “Customization Potential”- Custom Metalization: The paper uses photolithographic lift-off with strip patterns (50 µm pitch) and pixel metallizations for bump bonding to FE-I4 and CMS pixel ASICs. 6CCVD offers in-house metalization with Au, Pt, Pd, Ti, W, and Cu — enabling matched metallurgical stacks (e.g., Ti/Pt/Au for wire bonding, Ti/W for pixel bump-bonding compatibility).
- Geometry Customization: Strip, pixel, and 3D cell patterns can be fabricated to specification, including the ATLAS DBM 18 mm × 21 mm footprint or the CMS BCM1F geometry.
- Surface Preparation: 6CCVD’s polishing capabilities (Ra < 5 nm for inch-size PCD, Ra < 1 nm for SCD) support the surface quality required for low-leakage, high-uniformity detectors.
- Wafer Preselection & QC: 6CCVD supports pre-shipment characterization protocols including IV/CV curves, charge collection measurements, and visual inspection under crossed polarizers for stress and void mapping.
Engineering Support
Section titled “Engineering Support”- Material Selection Consultation: 6CCVD’s in-house PhD engineering team can assist with selecting the optimal diamond grade (SCD vs. PCD), thickness, and metalization scheme for high-radiation particle detection applications spanning planar pad, strip, pixel, and 3D electrode architectures.
- Prototype Development: From single-pixel test devices to full-size 10 cm2 3D pixel modules, 6CCVD supports iterative prototyping for HL-LHC-class detector R&D.
- Cryogenic Operation Guidance: For applications requiring diamond sensor operation at cryogenic temperatures (e.g., dipole cryostat beam loss monitors), 6CCVD can advise on material behavior and integration considerations.
Call to Action
Section titled “Call to Action”For custom specifications, advanced 3D cell fabrication, metalization stack design, or material consultation for radiation-hard tracking detector projects, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract
The RD42 collaboration at CERN is leading the effort to develop radiation tolerant devices based on polycrystalline Chemical Vapor Deposition (pCVD) diamond as a material for tracking detectors operating in harsh radiation environments. Diamond has properties that make it suitable for such detector applications. During the last few years the RD42 group has succeeded in producing and characterising a number of devices to address specific issues related to their use at the LHC and HL-LHC. Herein we present the status of the RD42 project with emphasis on recent beam test results and our proposed three year research plan. In particular, we review recent results on the stability of signal size on incident particle rate in diamond detectors over a range of particle fluxes up to 20 MHz/cm2, on the radiation tolerance of CVD diamond, on the diamond work with ATLAS and CMS, on the results of 3D diamond detectors fabricated in pCVD diamond and on the work with diamond manufacturers. In addition, we present the details of our proposed 3 year program including milestones.
Tech Support
Section titled “Tech Support”Original Source
Section titled “Original Source”- DOI: None