Hydrogen-terminated polycrystalline diamond MOSFETs with Al2O3 passivation layers grown by atomic layer deposition at different temperatures
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2018-06-01 |
| Journal | AIP Advances |
| Authors | Zeyang Ren, Guansheng Yuan, Jinfeng Zhang, Lei Xu, Jincheng Zhang |
| Institutions | Xidian University |
| Citations | 33 |
| Analysis | Full AI Review Included |
Hydrogen-Terminated Polycrystalline Diamond MOSFETs with Al2O3 Passivation
Section titled “Hydrogen-Terminated Polycrystalline Diamond MOSFETs with Al2O3 Passivation”Executive Summary
Section titled “Executive Summary”- Device Architecture: Hydrogen-terminated polycrystalline diamond MOSFETs utilizing ALD-grown Al2O3 passivation layers and a gold (Au) hard mask fabrication process.
- Material Advantage: Exploits the p-type surface conductivity of H-diamond to bypass the need for traditional dopants with low ionization energy.
- Process Variable: Two ALD deposition temperatures (200 °C and 300 °C) were systematically compared to optimize dielectric quality on polycrystalline diamond.
- Key Achievement: A maximum drain current of 339 mA/mm was achieved on a 2 µm gate-length device with 200 °C-grown Al2O3, representing one of the highest reported values for diamond MOSFETs without NO2 adsorption enhancement.
- Performance Trade-off: The 200 °C device exhibited superior output current, transconductance, and low on-resistance, while the 300 °C device demonstrated improved gate dielectric breakdown tolerance under forward bias.
- Leakage Mechanism: Gate forward leakage at high electric fields is governed by Frenkel-Poole (FP) emission.
- Forward Outlook: The authors propose a hybrid dielectric stack (200 °C Al2O3 + high-κ layer) as the pathway to next-generation high-stability, high-performance diamond MOSFETs.
Technical Specifications
Section titled “Technical Specifications”| Parameter | Value | Unit | Context |
|---|---|---|---|
| Substrate Type | Hydrogen-terminated polycrystalline diamond (H-PCD) | - | p-type surface conductivity channel |
| Gate Length (Lg) | 2 | µm | Device nominal dimension |
| Maximum Drain Current (IDS,max) | 339 | mA/mm | Achieved with 200 °C Al2O3 |
| Gate Dielectric | Al2O3 | - | Grown by Atomic Layer Deposition (ALD) |
| ALD Temperature (Sample A) | 200 | °C | High-performance variant |
| ALD Temperature (Sample B) | 300 | °C | High-stability variant |
| Maximum fT (literature) | 53 | GHz | H-diamond FET benchmark |
| Maximum fmax (literature) | 120 | GHz | H-diamond FET benchmark |
| Max Drain Current (literature) | 1.35 | A/mm | Highest reported H-diamond FET |
| Leakage Mechanism | Frenkel-Poole (FP) emission | - | Dominant at high E-field |
| Hard Mask Material | Gold (Au) | - | Used for device patterning |
Key Methodologies
Section titled “Key Methodologies”- Substrate Preparation: Started with polycrystalline diamond and applied hydrogen termination (H-diamond) to generate the 2DHG (two-dimensional hole gas) surface conductive layer.
- Gate Definition: Used a gold (Au) hard mask to pattern the gate region, avoiding plasma-induced damage to the H-diamond surface.
- Dielectric Deposition:
- Atomic Layer Deposition (ALD) of Al2O3.
- Sample A: 200 °C deposition temperature.
- Sample B: 300 °C deposition temperature.
- Electrical Characterization:
- Output characteristics (IDS-VDS) measured at VGS from -10 V to +7.4 V (Sample A).
- Transfer characteristics measured at VDS = -20 V.
- Gate diode I-V sweeps to identify leakage mechanisms (FP emission).
- Successive measurement cycles to verify operational stability.
- Failure Analysis: Extracted Schottky barrier inhomogeneity via Richardson’s plot, demonstrating reduced barrier height variation in the 200 °C film.
6CCVD Solutions & Capabilities
Section titled “6CCVD Solutions & Capabilities”- Applicable Materials: This research relies on high-purity Optical/Electronic Grade Polycrystalline Diamond (PCD) with pristine hydrogen-terminated surfaces. 6CCVD provides H-terminated PCD plates up to 125 mm in diameter, with controlled surface roughness (< 5 nm Ra) and thicknesses up to 500 µm, directly suitable for fabricating 2DHG devices.
- Customization Potential: The paper uses a Au hard mask and requires precise gate-length definition (2 µm). 6CCVD offers in-house precision laser cutting to deliver custom die dimensions and internal metalization services (Au, Ti, Pt, Pd, W, Cu) — including full Ti/Pt/Au stack deposition — to support H-diamond MOSFET fabrication workflows.
- Dielectric Integration Support: For the proposed Al2O3 / high-κ bilayer stack, surface preparation is critical. 6CCVD can supply diamond wafers with tailored termination (H-terminated or O-terminated) and customized surface prep protocols to optimize ALD nucleation on PCD films.
- Engineering Support: Our in-house PhD engineering team can assist with material selection, thickness optimization, and metalization stack design for high-power, high-frequency diamond MOSFET and MESFET projects. We support both R&D prototyping and scaled pilot production.
Call to Action: For custom specifications or material consultation, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract
Metal oxide semiconductor field effect transistors (MOSFETs) with Al2O3 passivation layer grown by atomic layer deposition (ALD) at 200 oC and 300 oC were fabricated on hydrogen-terminated polycrystalline diamond by using gold mask technology. The device with 200 oC grown Al2O3 dielectric shows high output current, low on-resistance, large threshold voltage and high transconductance compared to that with 300 oC grown Al2O3. A maximum drain current of 339 mA/mm has been achieved by the 2-μm device of the former kind, which, as we know, is the best result reported for the diamond MOSFETs with the same gate length except the NO2-adsorbed case. The current-voltage (I-V) of gate diodes of both kinds of devices show the gate forward leakage is dominated by the Frenkel-Poole (FP) emission mechanism at a high electric field, and the gate of the latter device can sustain higher forward bias. The stability of successive I-V measurements of both kinds of devices was proved. We expect that a high performance H-diamond MOSFET with high stability can be achieved by a double-layer dielectric structure with 200 oC grown Al2O3 stacked by another high-quality high κ dielectric.