Спектроскопические свойства полимерных пленок, активированных супрамолекулярным наноалмазным комплексом европия с батофенантролином

MetadataDetails
Publication Date2019-01-01
JournalЖурнал технической физики
AuthorsВ.А. Лапина, Т.А. Павич, П.П. Першукевич

For the first time, using the supramolecular diamond-containing europium (III) complex with bathophenanthroline, new luminescent films were obtained, converting UV radiation in the wavelength range of 220-410 nm with high efficiency to luminescence of europium ions, with the ability to control the degree of monochromaticity of radiation in the main emission band of Eu3+ ions with maximum of 615 nm. It was found that the shape of the excitation spectra, the half-width of the main emission band of 615 nm (transition 5D0-7F2), the values of quantum yields (within ~ 0.3-0.8) depend on the type of matrix material. The proposed optical materials can be used in the development of various light-emitting devices: screens, indicators, solar concentrators, organic light-emitting diodes, laser media.