CO2 reduction to formic acid at low overpotential on BDD electrodes modified with nanostructured CeO2

MetadataDetails
Publication Date2019-01-01
JournalJournal of Materials Chemistry A
AuthorsEnrico Verlato, Simona Barison, Yasuaki Einaga, Stefano Fasolin, Marco Musiani
InstitutionsKeio University, University of Bologna
Citations34

Nanostructured CeO<sub>2</sub>/BDD electrodes produce formic acid with good faradaic efficiency at very low overpotential (&gt;40% at <italic>Ī·</italic> ā‰ˆ 40 mV).