Abstract
Section titled āAbstractāQuantum technologies is attracting significant investment due to the range of potential applications, yet behind any new technology are enabling materials. Diamond is one such material, which has been used in demonstrations ranging from magnetic sensing to quantum computing. In order for these diamond quantum technologies to move from laboratory-based demonstrations to commercial products requires material with repeatable properties that can be produced with scale. This paper will focus on two diamond materials developed for magnetic sensing and quantum information processing. Specifically we will show the characterisation of high NV materials demonstrating repeatable properties such as T2* and low strain.