Femtosecond Laser Trimming of CVD-Diamond Coated Punch for Fine Embossing
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2019-11-14 |
| Journal | MATERIALS TRANSACTIONS |
| Authors | Tatsuhiko Aizawa, Tomomi Shiratori, Tomoaki Yoshino, Tadahiko Inohara |
| Institutions | Komatsu (Japan), Shibaura Institute of Technology |
| Citations | 9 |
| Analysis | Full AI Review Included |
Executive Summary
Section titled “Executive Summary”- Objective: Enhance precision metal forming (micro-embossing and piercing) by utilizing femtosecond laser machining to trim CVD-diamond coated WC(Co) punches.
- Material: A 9 µm thick polycrystalline CVD diamond coating applied to 2 mm diameter WC(Co) punches.
- Challenge Solved: Standard as-deposited diamond films exhibit high surface roughness (up to 1-3 µm) and geometric inaccuracies (initial shoulder curvature of 12 µm), making them unsuitable for fine stamping and forging.
- Methodology: Application of a femtosecond laser (180-190 fs pulse duration, 82W average power, 600 kHz max repetition) combined with a rotating jig to homogeneously trim both the side surface and the head of the cylindrical punch.
- Key Result: Successfully reduced the punch shoulder curvature from 12 µm down to 2.75 µm (an approximate 77% reduction).
- Performance Impact: Fine embossing of AISI304 sheets demonstrated a higher maximum applied load (Pmax = 465 N vs. 437 N) and a narrower affected zone along the shearing line, indicating superior plastic flow concentration and minimized elastic recovery.
- Significance: Establishes a flexible, precise post-treatment process for cylindrical and complex-shaped punches, facilitating dry technology without wet lubrication.
Technical Specifications
Section titled “Technical Specifications”| Parameter | Value | Unit | Context |
|---|---|---|---|
| Substrate Material | WC(Co) | - | Punch substrate (Tungsten Carbide with Cobalt binder). |
| Diamond Film Thickness | 9 | µm | Initial as-deposited coating thickness. |
| Punch Head Diameter | 2 | mm | Dimension of the cylindrical punch head. |
| Initial Shoulder Curvature | 12 | µm | Radius of the punch edge before laser treatment. |
| Final Shoulder Curvature | 2.75 | µm | Radius of the punch edge after femtosecond laser trimming. |
| Initial Surface Roughness | 1 - 3 | µm | Typical maximum roughness of standard CVD diamond films. |
| Laser Pulse Duration | 180 - 190 | fs | Femtosecond laser processing parameter. |
| Average Laser Power | 82 | W | Femtosecond laser processing parameter. |
| Max Repetition Rate | 600 | kHz | Femtosecond laser processing parameter. |
| Min Beam Spot Size | 1 - 10 | µm | Achieved using a fixed lens (1 µm) or Galvanometer (10 µm). |
| Max Scanning Speed | 3000 | mm/s | Femtosecond laser processing parameter. |
| Work Material | AISI304 | - | Stainless steel sheet used for embossing tests. |
| Sheet Thickness | 0.1 | mm | Thickness of the AISI304 workpiece. |
| Avg. Max Load (Untrimmed) | 437 (±4.2) | N | Average Pmax during embossing across 10 tests. |
| Avg. Max Load (Trimmed) | 465 (±7.5) | N | Average Pmax during embossing across 10 tests. |
| Raman Peak Positions | ~1330, ~1600 | cm-1 | Diamond (sp3) and Graphite (sp2) characteristic peaks. |
Key Methodologies
Section titled “Key Methodologies”- Substrate Preparation: Utilization of WC(Co) punches with a 2 mm head diameter as the base material.
- Diamond Coating: CVD (Chemical Vapor Deposition) process applied to grow a 9 µm thick polycrystalline diamond film directly onto the punch geometry.
- Laser Trimming Setup: Implementation of a rotating jig to ensure homogeneous ablation around the cylindrical punch side surface and head.
- Laser Parameters: Application of a femtosecond laser utilizing ultra-short pulses (180-190 fs) at a repetition rate up to 600 kHz to trim geometric inaccuracies without inducing significant thermal damage.
- Surface Analysis: Characterization via SEM (Scanning Electron Microscopy) to observe microstructural evolution and 3D laser microscopy to quantify the reduction in shoulder curvature.
- Material Integrity Check: Raman spectroscopy conducted to verify the nanostructure (sp3/sp2 ratio) of the diamond film post-ablation, ensuring the primary diamond structure remained unaffected.
- Performance Testing: Micro-embossing of 0.1 mm thick AISI304 sheets comparing trimmed versus untrimmed punches.
- Flow Analysis: EBSD (Electron Back-Scattering Diffraction) used to map the plastic strain distribution and phase transformations (γ-austenite) in the deformed AISI304 material.
6CCVD Solutions & Capabilities
Section titled “6CCVD Solutions & Capabilities”The transition from rough, as-deposited diamond films (1-3 µm roughness) to highly precise, sharp-edged tooling (2.75 µm curvature) required for advanced metal forming requires exact material specifications. 6CCVD provides the foundational materials to replicate or improve upon this research.
| Research Requirement | Recommended 6CCVD Capability |
|---|---|
| High-Wear Tooling Substrate | Optical Grade SCD or Standard PCD wafers. For tooling inserts requiring extreme hardness, our Polycrystalline Diamond (PCD) ensures the necessary durability for WC(Co) composite substrates. |
| Dimensional Precision | We provide custom PCD plates and wafers up to 125mm, allowing for precision machining of complex cylindrical punch arrays rather than standard sizes. |
| Surface Finish Requirement | The paper highlights a struggle with high roughness (1-3 µm). Our in-house polishing capabilities offer Ra < 5nm for Inch-size PCD, providing a superior starting baseline and reducing the laser trimming burden. |
| Film Thickness Control | We offer PCD thicknesses ranging from 0.1µm to 500µm, perfectly accommodating the specific 9 µm requirement or tailored thicknesses for varying forming loads. |
| Geometric Customization | Achieving a 2.75 µm edge curvature requires post-processing. 6CCVD provides custom laser cutting and shaping services to deliver diamond tooling geometries ready for femtosecond laser fine-tuning. |
| Material Consultation | For complex micro-embossing, piercing, or forging projects requiring tailored diamond solutions, our in-house PhD engineering team can assist with material selection to optimize tool life and minimize elastic recovery in formed parts. |
Applicable Materials:
- Heavy Polycrystalline Diamond (PCD): For maximum wear resistance on WC(Co) composite punches used in dry, high-stress metal forming.
- Optical Grade Single Crystal Diamond (SCD): For applications requiring sub-nanometer surface finishes prior to laser trimming.
Customization Potential: To extend this research, 6CCVD can provide PCD-coated or solid PCD punches with custom metalization (Ti, W, or Au) for brazier integration into forming assemblies. Our global shipping capabilities (DDU or DDP) ensure these custom diamond tooling components can be securely delivered to research facilities worldwide.
Engineering Support: 6CCVD’s in-house PhD team can assist with material selection for specific micro-embossing and fine piercing projects, ensuring the correct diamond grade and thickness is chosen to maximize load capacity and minimize material deformation.
Call to Action: For custom specifications, material consultation, or advanced tooling integration, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract
Femtosecond laser machining was employed to trim the surface roughness of diamond coating and to sharpen the edge corner of diamond coated punch toward fine piercing and embossing processes in metal forming. CVD-diamond coated WC (Co) punches with the head diameter of 2 mm were prepared for this laser-trimming process. The initial coated diamond film was 9 µm thick; the curvature of coated punch shoulder was 12 µm. The rotating jig was utilized to attain the homogeneous trimming of punch side surface as well as punch head. SEM (Scanning Electron Microscopy) and Raman spectroscopy were employed to describe the microstructure evolution with trimming as well as the effect of trimming on the nanostructure of diamonds. Fine embossing process into 0.1 mm thick AISI304 sheets with narrow clearance, was utilized to describe their plastic flow around the punch shoulder as well as the geometric distortion by elastic recovery. In addition, EBSD (Electron Back-Scattering Diffraction) was also employed to analyze the difference in plastic flow of AISI304 sheets during micro-embossing between the untrimmed and trimmed punches. The applied load to stroke relation, the plastic strain distribution and the phase mapping as well as the shear droop were compared between two diamond-coated punches to investigate the effect of laser-trimming on the quality of embossed product.