Femtosecond laser direct writing of high-performance structures and their applications
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2019-01-01 |
| Authors | Yasuhiko Shimotsuma, Torataro Kurita, Nobuya Mineyuki, Masahiro Shimizu, Kiyotaka Miura |
| Institutions | Kyoto University |
Abstract
Section titled āAbstractāDirect three-dimensional laser writing of functional microstructures in material was demonstrated. We demonstrated self-assembled periodic nanostructures in bulk semiconductor crystals and generation of ensemble nitrogen-vacancy (NV) centers inside a diamond.