Phonon assisted photoluminescence up-conversion of in diamond color centers

MetadataDetails
Publication Date2019-01-01
AuthorsJun Zhang, Yuanfei Gao, Yujia Sun
InstitutionsInstitute of Semiconductors, Chinese Academy of Sciences

Phonon assisted anti-Stokes photoluminescence (ASPL) up-conversion plays an important role in laser cooling of lattice phonon and controlling of electron and phonon states in solids. Here, we will introduce the phonon-assisted PL up-conversion process from nitrogen vacancy (NV) and silicon vacancy (SiV) center in diamond.