Physical Properties of Photonic Cooper Pairs Generated via Correlated Stokes–anti‐Stokes Raman Scattering
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2019-06-11 |
| Journal | physica status solidi (b) |
| Authors | Filomeno S. de Aguiar Júnior, C. H. Monken, Marcelo F. Santos, Reinaldo de Melo e Souza, André Saraiva |
| Institutions | Universidade Federal de Minas Gerais, Fundação Instituto de Pesca do Estado do Rio de Janeiro |
| Citations | 6 |
Abstract
Section titled “Abstract”The theoretical and experimental background for the creation of photonic Cooper pairs (PCPs) via correlated Stokes-anti‐Stokes Raman scattering is introduced, followed by experimental results on the second‐order photon time correlation g 2 (0) in diamond. It is shown how g 2 (0) changes with energy (Stokes-anti‐Stokes Raman shift), momentum (scattering angle) and excitation laser power. Both real and virtual phonon‐mediated scattering processes are addressed.