Diamond nanofocusing refractive X-ray lenses made by planar etching technology

MetadataDetails
Publication Date2019-08-01
JournalJournal of Synchrotron Radiation
AuthorsMikhail Lyubomirskiy, Pit Boye, Jan M. Feldkamp, Jens Patommel, Sebastian Schöeder
InstitutionsUniversitÀt Hamburg, Technische UniversitÀt Dresden
Citations9

The manufacturing steps and first tests of a refractive lens made of polycrystalline diamond are described. A fabrication process based on electron-beam lithography and deep reactive ion etching is introduced. Experimental tests on beamline ID13 at the ESRF have been performed. A spot size of 360 nm (FWHM) at an energy E = 24.3 keV is observed.