Skip to content

Low Temperature Growth of CVD Nanocrystalline Diamond Thin Film by Designed SWP-CVD with Various Working Pressures

MetadataDetails
Publication Date2019-09-01
JournalNanoscience and Nanotechnology Letters
AuthorsYeong Min Park, Moon Ki Han, Mun Ki Bae, Tae Gyu Kim

Nanocrystalline diamond (NCD) is exceptionally useful for a variety of applications and is of significant interest to researchers in technological and scientific fields due to its excellent mechanical and chemical properties, such as its hardness and high thermal conductivity. We have modified a microwave plasma chemical vapor deposition (MPCVD; Astex Inc.) system with a slot antenna designed for surface wave plasma (SWP) and successfully fabricated high quality thin NCD film. This SWP-CVD process fabricates high quality diamond film at 300 °C, while a normal MPCVD process requires the temperature of the substrate to be above 800 °C. We studied the fabricated NCD samples in detail, measuring their surface morphology by field emission scanning electron microscopy (FESEM); their structural-chemical properties by Raman spectroscopy; and their surface roughness by atomic force microscopy (AFM).