Acoustic diamond resonators with ultra-small mode volumes
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2020-01-01 |
| Authors | MikoÅaj K. Schmidt, Christopher G. Poulton, M. J. Steel |
| Institutions | University of Technology Sydney, Macquarie University |
| Citations | 1 |
Abstract
Section titled āAbstractāWe introduce a novel acoustic cavity for a high-cooperativity orbit-phonon coupling with color centers in diamond. The enhancement of coupling is achieved by localizing the energy of a GHz acoustic mode into a deep-subwavelength volume.