Cu4MnGe2S7 and Cu2MnGeS4 - two polar thiogermanates exhibiting second harmonic generation in the infrared and structures derived from hexagonal diamond
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2021-01-01 |
| Journal | Dalton Transactions |
| Authors | Jennifer R. Glenn, Jeong Bin Cho, Yiqun Wang, Andrew J. Craig, JianāHan Zhang |
| Institutions | Sogang University, Duquesne University |
| Citations | 16 |
Abstract
Section titled āAbstractāThe synthesis, structure, and physicochemical characterization of two diamond-like semiconductors are reported. Both compounds display second harmonic generation, bandgaps around 2 eV and wide windows of optical transparency in the infrared.