Multidisciplinary Materials Research at Harbin Institute of Technology
At a Glance
Section titled âAt a Glanceâ| Metadata | Details |
|---|---|
| Publication Date | 2021-02-01 |
| Journal | Advanced Materials |
| Authors | Shaoqin Liu, Bin Guo, Yu Zhou |
| Institutions | Harbin Institute of Technology |
Abstract
Section titled âAbstractâThis Special Issue of Advanced Materials, commemorating the 100th anniversary of Harbin Institute of Technology (HIT) is a collection of Reviews and Progress Reports articles by the faculty members and alumni of HIT, introducing the most innovative multidisciplinary research activities including materials science and engineering at HIT. Founded in 1920, Harbin Institute of Technology (HIT) has developed into an open, multidisciplinary, research-oriented, leading national university with science and engineering as its core. HIT has formed the pattern of âOne University, Three CampusesâHarbin Campus, Weihai Campus, and Shenzhen Campusâ (Figure 1). From âthe Cradle of Engineersâ to âInternational First-Rate Innovative Talentsâ as its goal, HIT has always been at the forefront of modern technology and national development. In 1954, Harbin Institute of Technology (HIT) became one of the Chinese top-six leading universities. In 1996, Harbin Institute of Technology (HIT) was the first batch of universities included in the Project 211 list. In 1999, Harbin Institute of Technology (HIT) became one of the top-nine key universities to be preferentially built according to the standards of internationally renowned universities. In 2009, Harbin Institute of Technology (HIT) became a member of the top-nine University Union (C9) in China. In 2017, HIT was included in the first batch of universities on the list of the Double First-Class initiative; 17 disciplines became Double First-Class disciplines. Currently, HIT has 20 schools, 2 affiliated hospitals, 10 national key laboratories, and 4 national engineering research centers. The university jointly with China Aerospace Science and Technology Corporation built a national âbig science facilityââthe Space Environment Simulation Research Infrastructure (SESRI) and a Collaborative Innovation Center of Astronautical Science and Technology. HITâs education system particularly emphasizes âStrictest Standard, Greatest Effortâ, providing students with a wide range of vigorous training. Therefore, HIT has cultured a large number of world-renowned scientists and engineers, and achieved a serials of âfirstsâ in scientific research and technology innovation in the past years, such as Chinaâs first simulation computer, the first intelligent chess-playing computer, the first arc-welding robots, the first world advanced-level system radar, the first CMOS-chip IC card, the first Chinese satellite-Earth high-speed laser communication test, the first giant computer-aided real-time 3D image construction system, the first microcomputer-operated fiber twiner, and the first large-scale tank-head-forming machine, independently developing 7 satellites in China etc. The famous âShenzhou Series Spaceship Projectâ received massive assistance from HIT in the field of large-scale land-based space-simulation equipment, returning cabin deformation and orthopraxy welding technology, a three-axel simulation experimental platform, and fault diagnosis. In a 2020 US News & World Report, HIT was ranked 6th in the list of Best Global Universities for Engineering. The field of materials science and engineering is the most rigorous one at HIT, and involves cutting-edge, interdisciplinary, and applied research. According to the Essential Science Indicators (ESI) by Clarivate Analytics, materials science research at HIT was ranked 9th in the world when considering the number of publications in 2010-2020, and 25th considering citations. According to a 2020 US News & World Report, HIT was ranked 40th in a list of Best Global Universities for Materials Science. This Special Issue of Advanced Materials features 10 Reviews and 14 Progress Reports, with major attention paid to the fields of materials design, fabrication and characterization, catalytic materials, solar-energy materials, energy-storage materials, composite materials, smart materials and flexible electronics, and biomaterials/biomimetics. In the field of materials design, Prof. Jiecai Han and Prof. Jiaqi Zhu summarize the research progress of diamond color centers based on the problems faced in the application of diamond color centers (article number 2000891). Prof. Guanying Chen provides an account of the recent progress on the conceptual design of bright lanthanide-doped near-infrared nanoparticles as well as their cutting-edge biophotonics applications ranging from single nanoparticle imaging to deep-tissue theranostics (article number 2000678). Prof. Zuhuang Chen highlights the recent progress on topological structures in the ferroic thin films and heterostructures (article number 2000857). Prof. Liang Zhen and Prof. Cheng-Yan Xu summarize the recent progress on electrochemical intercalation of foreign species into atomically thin 2D materials for structural phase transitions and device applications (article number 2000581). In the field of materials fabrication and characterization, Prof. Bin Guo surveys the recent progress of micro/nanoforming techniques for fabricating 3D metallic structures (article number 20200893). Prof. Shumin Xiao provides an account of recent progress on the patterning and integration techniques of micro- and nanostructured perovskites for optoelectronic and photonic applications (article number 2000306). In the field of catalytic materials, the progress report by Prof. Gang Wu aims to highlight important but challenging electrocatalysis associated with sustainable water (oxygen evolution and reduction reactions) and nitrogen (nitrogen reduction and ammonia oxidation reactions) cycles for energy and environmental sustainability (article number 2000381). Prof. Bo Song outlines the recent advances in design and modulation strategies of 2D transition-metal dichalcogenides for the hydrogen evolution reaction (HER) (article number 1907818). Dr. Yuyan Shao, Dr. Lei Du, and Prof. Yong Wang review the current understanding of degradation of low-platinum-group-metal (PGM) and PGM-free catalysts in proton-exchange-membrane (PEM) fuel cells and the progress on materials-based solutions (article number 1908232). In the field of solar energy materials, Prof. Zhiyong Tang outlines the state-of-the-art progress in asymmetric photocatalysis by heterogeneous nanomaterials (article number 202001731). Prof. Ping Xu provides a comprehensive review on surface-plasmon-assisted/enhanced electrocatalysis and photocatalysis (article number 2000086). In the field of energy-storage materials, Prof. Chunsheng Wang reviews recent advances and gives perspective on all-solid-state Li/S batteries using sulfide solid electrolytes (article number 2000751). Prof. Jiajun Wang highlights the interface issues, solutions, and recent developments of solid-state batteries for next-generation electrochemical energy storage (article number 2000721). Prof. Kai He outlines the recent development of in situ electron microscopy for rechargeable ion batteries (article number 2000699). In the field of composite materials, Prof. Lujun Huang and Prof. Lin Geng provide a comprehensive review on smart multiscale architecture and superior performance of titanium matrix composites (article number 202000688). Prof. Yibin Li outlines the recent progress on graphene/polymer nanocomposites for multifunctional applications (article number 2001105). In the field of smart materials, Prof. Jinsong Leng provides a comprehensive review on the mechanisms and applications of shape-memory polymers and composites, and highlights the design and regulation of the shape-memory effect for prospective applications (article number 2000713). Prof. Yuyan Liu provides an account of the recent progress on surface-wetting control and practical applications based on superwetting shape-memory microstructures (article number 2001718). In the field of flexible electronics, Prof. PingAn Hu gives a comprehensive review on atomically thin hexagonal boron nitride and its heterostructures for electronic and optoelectronic devices (article number 2000769). Prof. Yudong Huang highlights the importance of structure design and chemical modification of poly(dimethylsiloxane) (PDMS) substrates for stretchable electronics (article number: 2003155). In the field of biomaterials/biomimetics, Prof. Shaoqin Liu summarizes recent advances in using various nanomaterials for facilitating microbial extracellular electron transfer processes occurring at both the bacteria-electrode interface and the biotic interface (article number 2004051). Prof. Qiang He and Prof. Xing Ma outline the recent progress of biomedical micro-/nanomotors toward overcoming biological barriers and in vivo imaging (article number 2000512). Prof. Xiaojun Han provides a comprehensive review on functional artificial cells/tissues based on versatile phospholipid assemblies (article number 2002635). Prof. Yao Li gives a comprehensive review on bioinspired microstructured materials for optical and thermal regulation (article number 2000697). In this issue, we introduce the multidisciplinary research activities at HIT; although the issue cannot cover all the materials research at HIT. We sincerely hope that this Special Issue will inspire readers to pay close attention to discover more research breakthroughs at HIT beyond this publication, and will stimulate more exciting collaborations. We are grateful to Dr. Peter Gregory, Dr. Emily Xiaoge Hu, and the editorial team of Advanced Materials for their great efforts in making this issue a reality. The full support from HIT has also been vital for the publication. Finally, we sincerely thank all the co-authors for their important contributions to this Special Issue. Shaoqin Liu received her Bachelorâs degree from Wuhan University of Hydraulic and Electric Engineering in 1994 and her Ph.D degree from Changchun Institute of Applied Chemistry (Chinese Academy of Science) in 1999. She started her chemistry research career in Professor Shaojun Dongâs group at Changchun Institute of Applied Chemistry, developing polyoxometalate-based thin films. After her Ph.D degree, she moved to the Max-Planck-Institute of Colloids and Interface as a Humboldt Fellow where she developed polyoxometalate-based functional materials. In 2004, she joined the National Research Council of Canada as an NESRC fellow to study direct methanol fuel cells. In 2007, she started her academic career as a Full Professor in Harbin Institute of Technology. Her current research interests include preparation of nanostructured materials and their applications in energy, biosensing, and cancer therapy. Bin Guo has been a full professor in the School of Materials Science and Engineering at Harbin Institute of Technology (HIT) from 2001. He is currently the vice present of HIT and the director of the Key Laboratory of Microsystems and Microstructured Manufacturing of Ministry of Education, China. He received his B.S., M.S., and Ph.D. degrees from HIT in 1983, 1985, and 1991, respectively. He was a senior visiting scholar at Chiba Institute of Technology from 1993 to 1998. His current interests focus on innovative micro-/nanomanufacturing processes and systems, particularly in the areas of deformation-based processes and laser processes. Yu Zhou has been engaged in the area of ceramics and ceramic-matrix composites (CMCs) for 35 years, mainly focusing on the development of multifunctional thermal ceramics and near-net forming technologies for special-shaped or large-sized ceramic components. He has been the President of Harbin Institute of Technology (HIT) since 2014. He received his B.S., M.S., and Ph.D. degrees from HIT in 1982, 1984, and 1989, respectively.