“Quantum sensor” assisted magnetic resonance

MetadataDetails
Publication Date2021-03-18
AuthorsAshok Ajoy
InstitutionsUniversity of California, Berkeley

The development of point-like quantum sensors based on wide bandgap materials, in particular the Nitrogen Vacancy (NV) center in diamond, has thrown up exciting new possibilities for the NMR of materials, molecules, and biological systems through optical means. I will describe how NV center endowed nanodiamonds could usher in a new form of a “deployable” NMR sensor with novel applications to signal enhanced NMR spectroscopy and imaging.