Theoretical investigation of charge transfer between the NV− center in diamond and substitutional N and P
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2021-10-15 |
| Journal | Journal of Applied Physics |
| Authors | Rodrick Kuate Defo, Xingyu Zhang, Steven L. Richardson, Efthimios Kaxiras |
| Institutions | Harvard University, MIT Lincoln Laboratory |
| Citations | 6 |
Abstract
Section titled “Abstract”The nitrogen-vacancy (NV) lattice defect in diamond, consisting of an N substitutional atom and an adjacent C vacancy, is commonly observed in two charge states, negative (NV−) and neutral (NV0). The NV− defect exhibits spin state-dependent fluorescence and is, therefore, amenable to optical methods for spin-state readout, while the NV0 is not. Hence, the NV− defect is much more useful for quantum sensing and quantum information processing. However, only NV0 electroluminescence has been observed, even from centers showing NV− in photoluminescence. In the present work, we use first-principles electronic structure calculations to determine adiabatic charge transition levels for the conversion of NV− to NV0 in the presence of substitutional N or P impurities, which provide the charge of the NV− center. We find that the adiabatic charge transition levels in the presence of such impurities lie at energies close to or lower than the zero-phonon line of the NV− center and that these energies only decrease as the concentration of N donors increases. This work, therefore, elucidates the absence of observed electroluminescence from the NV− and proposes a path toward observation of the phenomenon.