Nitrogen investigation by SIMS in two wide band-gap semiconductors - Diamond and Silicon Carbide

MetadataDetails
Publication Date2021-11-26
JournalHAL (Le Centre pour la Communication Scientifique Directe)
AuthorsM.A. Pinault-Thaury, M.A. Pinault-Thaury, François Jomard
InstitutionsGroupe d’Étude de la Matière Condensée

Diamond and Silicon Carbide (SiC) are promising wide band-gap semiconductors for power electronics, SiC being more mature especially in term of large wafer size (that has reached 200 mm quite recently). Nitrogen impurities are often used in both materials for different purpose: increase the diamond growth rate or induce n-type conductivity in SiC. The determination of the nitrogen content by secondary ion mass spectrometry (SIMS) is a difficult task mainly because nitrogen is an atmospheric element for which direct monitoring of N$^\pm$ ions give no or a weak signal. With our standard diamond SIMS conditions, we investigate 12C14N-secondary ions under cesium primary ions by applying high mass resolution settings. Nitrogen depth-profiling of diamond and SiC (multi-) layers is then possible over several micrometer thick over reasonable time analysis duration. In a simple way and without notably modifying our usual analysis process, we found a nitrogen detection limit of $2\times 10^{17}$ at/cm$^3$ in diamond and $5\times10^{15}$ at/cm$^3$ in SiC.