Abstract
Section titled âAbstractâStructural optimization is a methodology used to generate novel structures within a design space by finding a maximum or minimum point within a set of constraints. Topology optimization, as a subset of structural optimization, is often used as a means for light-weighting a structure while maintaining mechanical performance. This article presents the mathematical basis for topology optimization, focused primarily on the Bi-directional Evolutionary Structural Optimization (BESO) and Solid Isotropic Material with Penalization (SIMP) methodologies, then applying the SIMP methodology to a case study of additively manufactured lattice cells. Three lattice designs were used: the Diamond, I-WP, and Primitive cells. These designs are all based on Triply Periodic Minimal Surfaces (TPMS). Individual lattice cells were subjected to a uniaxial compression load, then optimized for these load conditions. The optimized cells were then compared to the base cell designs, noting changes in the stress field response, and the maximum and minimum stress values. Overall, topology optimization proved its utility under this loading condition, with each cell seeing a net gain in performance when considering the volume reduction. The I-WP lattice saw a significant stress reduction in conjunction with the mass and volume reduction, marking a notable increase in cell performance.
Tech Support
Section titled âTech SupportâOriginal Source
Section titled âOriginal SourceâReferences
Section titled âReferencesâ- 2016 - Additive manufacturing of metallic components by selective electron beam melting â a review [Crossref]
- 2018 - Topology-mechanical property relationship of 3D printed strut, skeletal, and sheet based periodic metallic cellular materials [Crossref]
- 2019 - On mechanical properties of cellular steel solids with shell-like periodic architectures fabricated by selective laser sintering [Crossref]
- 2019 - Multifunctional mechanical metamaterials based on triply periodic minimal surface lattices [Crossref]
- 2020 - Survivability and damage modeling of advanced materials
- 2021 - First cell failure of lattice structure under combined loading
- 2015 - Topology optimization of lightweight periodic lattices under simultaneous compressive and shear stiffness constraints [Crossref]