Record-Low Thermal Boundary Resistance between Diamond and GaN-on-SiC for Enabling Radiofrequency Device Cooling
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2021-12-07 |
| Journal | ACS Applied Materials & Interfaces |
| Authors | Mohamadali Malakoutian, D. Field, Nicholas Hines, Shubhra S. Pasayat, Samuel Graham |
| Institutions | University of Bristol, Georgia Institute of Technology |
| Citations | 98 |
| Analysis | Full AI Review Included |
Executive Summary
Section titled “Executive Summary”- Record-Low Thermal Boundary Resistance (TBR): Achieved a TBR of 3.1 ± 0.7 m2 K/GW at the diamond/Si3N4/GaN interface, the closest to theoretical prediction (Diffuse Mismatch Model) reported to date.
- Atomically Close Integration: Successfully integrated polycrystalline diamond (PCD) within ~1 nm of the GaN channel layer without degrading the 2-dimensional electron gas (2DEG) electrical properties (mobility and sheet carrier concentration remained stable).
- High Thermal Conductivity Diamond: The 2 µm PCD layer demonstrated a thermal conductivity (TC) of 638 ± 48 W/m·K with a ~1.9 µm lateral grain size, enabling highly efficient vertical and lateral heat spreading.
- Optimized Nucleation Stage: Detailed a specific chemical vapor deposition (CVD) nucleation recipe to minimize the interfacial layer thickness, reducing the total channel thermal resistance to ~6.2 m2 K/GW.
- Application Focus: Validated as a critical thermal management solution for 5G-and-beyond GaN radiofrequency (RF) high electron mobility transistors (HEMTs) facing severe self-heating challenges at high power densities (e.g., 40 W/mm at X-band, 8 W/mm at W-band).
Technical Specifications
Section titled “Technical Specifications”| Parameter | Value | Unit | Context |
|---|---|---|---|
| Thermal Boundary Resistance (TBR) | 3.1 ± 0.7 | m2 K/GW | Diamond / Si3N4 / GaN interface (Record low) |
| Overall Channel Thermal Resistance | ~6.2 | m2 K/GW | Combined diamond and boundary resistance |
| Diamond Thermal Conductivity (TC) | 638 ± 48 | W/m·K | Measured via Transient Thermoreflectance (TTR) |
| Diamond Lateral Grain Size | ~1.9 | µm | Polycrystalline diamond (PCD) |
| Diamond Film Thickness | >2.0 | µm | Polycrystalline diamond layer |
| Nucleation Layer Thickness | <30 | nm | Ultrananocrystalline diamond (UNCD) layer |
| Remaining Si3N4 Layer Thickness | ~1 | nm | Interfacial dielectric layer |
| GaN Channel Mobility (µn) | 1235 | cm2 /V·s | Post-diamond growth (Reference: 1250) |
| Sheet Carrier Concentration (ns) | 1.36 × 1013 | cm-2 | Post-diamond growth (Reference: 1.35 × 1013) |
| Sheet Resistivity (ρs) | 373 | Ω/▣ | Post-diamond growth (Reference: 370) |
| Plasma Power (Nucleation) | 600 | W | Microwave Plasma CVD (MPCVD) parameter |
| Chamber Pressure (Nucleation) | 20 | Torr | MPCVD parameter |
| CH4 Concentration (Nucleation) | 5 | % | Optimized to minimize damage |
| Nucleation Time | 10 | min | Optimized recipe duration |
| Growth Temperature | ~700 | °C | Surface temperature during deposition |
Key Methodologies
Section titled “Key Methodologies”- Substrate Preparation: Utilized N-polar GaN HEMT structures on SiC and Sapphire substrates, coated with a 5-10 nm MOCVD-deposited Si3N4 thermal interface layer.
- Diamond Nucleation Stage: Exposed the Si3N4/GaN surface to H2/CH4 plasma via Microwave Plasma Chemical Vapor Deposition (MPCVD) using a highly controlled recipe (600 W, 20 Torr, 5% CH4, 10 min).
- Interfacial Conversion: Allowed for carbon diffusion to replace nitrogen atoms near the Si3N4 surface, forming a thin interfacial SiC layer to enhance phonon transport and diamond adhesion.
- Diamond Growth Stage: Transitioned to standard CVD growth to increase grain size from <50 nm (UNCD) to ~1.9 µm (NCD/MCD) while maintaining the channel’s electrical integrity.
- Characterization:
- STEM / EELS / EDS: Analyzed cross-sectional interfacial layer thicknesses and elemental composition.
- Hall Effect Measurements: Verified 2DEG mobility and sheet carrier concentration.
- Transient Thermoreflectance (TTR): Measured diamond thermal conductivity and thermal boundary resistance.
6CCVD Solutions & Capabilities
Section titled “6CCVD Solutions & Capabilities”-
Applicable Materials: To replicate the thermal conductivity and interface engineering required for this study, Optical Grade Polycrystalline Diamond (PCD) with controlled large-grain sizes (~1-2 µm) is required. For ultimate device cooling applications requiring higher thermal pathways or alternative integration schemes, Optical Grade Single Crystal Diamond (SCD) substrates can also be provided. Our MPCVD-grown PCD matches the necessary thickness ranges (0.1 µm to 500 µm) and supports grain sizes optimized for high thermal flux transport.
-
Customization Potential: The research highlights the critical need for extreme precision in interfacial layers and thermal boundary management. 6CCVD specializes in custom-dimension PCD plates/wafers up to 125mm, allowing us to tailor polycrystalline diamond for specific GaN-on-SiC or GaN-on-Sapphire templates. Furthermore, our in-house metallization capabilities support custom metal stack depositions (e.g., Ti/Pt/Au) if direct die-attach or wire-bonding thermal characterization setups are required, alongside precision laser cutting for specific device geometries.
-
Engineering Support: Integrating wide bandgap materials such as GaN and Diamond involves navigating severe lattice mismatch, residual stress, and plasma-induced damage. 6CCVD’s in-house PhD engineering team is uniquely equipped to assist with material selection, grain-size optimization, and nucleation layer engineering for advanced GaN RF Device Cooling and High-Power 5G HEMT projects. We can help optimize your MPCVD recipes to achieve sub-30nm nucleation layers and highly isotropic polycrystalline diamond growth.
-
Call to Action: For custom specifications, substrate consultation, or material selection for your next-generation thermal management research, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract
The implementation of 5G-and-beyond networks requires faster, high-performance, and power-efficient semiconductor devices, which are only possible with materials that can support higher frequencies. Gallium nitride (GaN) power amplifiers are essential for 5G-and-beyond technologies since they provide the desired combination of high frequency and high power. These applications along with terrestrial hub and backhaul communications at high power output can present severe heat removal challenges. The cooling of GaN devices with diamond as the heat spreader has gained significant momentum since device self-heating limits GaN’s performance. However, one of the significant challenges in integrating polycrystalline diamond on GaN devices is maintaining the device performance while achieving a low diamond/GaN channel thermal boundary resistance. In this study, we achieved a record-low thermal boundary resistance of around 3.1 ± 0.7 m<sup>2</sup> K/GW at the diamond/Si<sub>3</sub>N<sub>4</sub>/GaN interface, which is the closest to theoretical prediction to date. The diamond was integrated within ∼1 nm of the GaN channel layer without degrading the channel’s electrical behavior. Furthermore, we successfully minimized the residual stress in the diamond layer, enabling more isotropic polycrystalline diamond growth on GaN with thicknesses >2 μm and a ∼1.9 μm lateral grain size. More isotropic grains can spread the heat in both vertical and lateral directions efficiently. Using transient thermoreflectance, the thermal conductivity of the grains was measured to be 638 ± 48 W/m K, which when combined with the record-low thermal boundary resistance makes it a leading-edge achievement.