Electron microscopy of gallium nitride growth on polycrystalline diamond
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2015-10-15 |
| Journal | Semiconductor Science and Technology |
| Authors | Richard F. Webster, D. Cherns, Martin Kuball, Quanbo Jiang, D.W.E. Allsopp |
| Institutions | University of Bristol, University of Bath |
| Citations | 21 |
| Analysis | Full AI Review Included |
Executive Summary
Section titled “Executive Summary”- Heterostructure Engineering: This study demonstrates the growth of gallium nitride (GaN) high electron mobility transistor (HEMT) structures on polycrystalline diamond (PCD) substrates, achieving (0001)-oriented epitaxial layers despite a ~13% lattice mismatch between GaN and diamond.
- Low-Temperature Nucleation: A low-temperature aluminum nitride (AlN) buffer layer (~70 nm) was successfully used to promote GaN nucleation directly on the polycrystalline diamond surface, resolving the lack of a fixed epitaxial relationship.
- Dislocation Density Reduction: Unmasked growth initially yielded threading dislocation (TD) densities of ~7 × 109 cm−2, which were reduced by a factor of ~3 from the bottom to the top of the 1.5 µm film through surface step migration.
- ELOG Technique Success: Epitaxial Layer Overgrowth (ELOG) using SixNy masks combined with ICP etching reduced TD densities by two orders of magnitude, achieving <108 cm−2 in lateral overgrowth regions, with dislocation-free zones above the masked areas.
- Thermal Management Driver: Diamond’s exceptional thermal conductivity (~2000 W·m−1·K−1) motivates its use as a heat-spreading substrate for GaN power electronics, offering a pathway to lower operating temperatures and longer device lifetimes compared to sapphire, Si, or SiC substrates.
- Crack Mitigation Challenge: Observed 60° cracking along (10-10) planes results from the large CTE mismatch (diamond: 4.38 × 10−6 K−1; GaN: 5.59 × 10−6 K−1), placing GaN in tensile stress during cooldown.
- Substrate Economics: Polycrystalline CVD diamond provides a cost-effective alternative to single crystal diamond for thermal management in wide-bandgap device applications.
Technical Specifications
Section titled “Technical Specifications”| Parameter | Value | Unit | Context |
|---|---|---|---|
| Diamond Thermal Conductivity | ~2000 | W·m−1·K−1 | Single crystal benchmark cited for motivation |
| PCD Grain Size | 1-2 | µm | Substrate microstructure |
| GaN Lattice Mismatch to Diamond | ~13 | % | Drives defect formation |
| Diamond CTE | 4.38 × 10−6 | K−1 | Thermal expansion coefficient |
| GaN CTE | 5.59 × 10−6 | K−1 | Thermal expansion coefficient |
| Thermal Cleaning Temperature | ~1000 | °C | 10 min pre-growth anneal |
| AlN Monolayer Formation Temp | ~650 | °C | Aluminum monolayer deposition |
| AlN Buffer Layer Thickness | 70 | nm | Nucleation layer |
| AlN Growth Pressure | 100 | mbar | MOVPE reactor condition |
| NH3 Flow Rate | ~1200 | sccm (SLM) | MOVPE gas chemistry |
| TMAl Flow Rate | ~23 | sccm (SLM) | Metalorganic precursor |
| H2 Carrier Flow Rate | ~4.5 | sccm (SLM) | Carrier gas |
| GaN Layer Thickness | 1.5 | µm | Active HEMT buffer |
| AlN Spacer Layer Thickness | ~2 | nm | Interlayer between GaN and barrier |
| AlGaN Barrier Thickness | 20 | nm | HEMT top barrier |
| GaN Growth Temperature | 1060 | °C | MOVPE deposition |
| Initial Threading Dislocation Density | ~7 × 109 | cm−2 | Unmasked sample |
| ELOG TD Density | <108 | cm−2 | Lateral overgrowth region |
| Hillock Width | 15 | µm | Lateral GaN island dimension |
| Misorientation Between Hillocks | ±3 to 6 | ° | Crystallographic tilt |
| Ni Etch Mask Thickness | ~200 | nm | ICP etch mask for ELOG patterning |
| GaN Stripe Orientation | (10-10) | Plane | ELOG sidewall facet |
| GaN Polarity | N-polar | — | Determined by CBED |
| FIB Pt Protective Layer | 2 | µm | TEM sample prep |
| FIB Rough Milling Voltage | 30 | kV | Ga ion beam |
| FIB Polishing Voltage | 5 | kV | Low-kV final thinning |
| TEM Operating Voltage | 200 / 160 | kV | Philips EM430 / JEOL 2010 |
Key Methodologies
Section titled “Key Methodologies”- Substrate Preparation: Polycrystalline diamond substrates grown by plasma-assisted CVD on Si, with 1-2 µm grain size; thermal cleaning at ~1000 °C for 10 min prior to epitaxy.
- AlN Nucleation Layer Deposition: Formation of Al monolayer at ~650 °C, followed by AlN growth at 100 mbar with NH3 (~1200 sccm), TMAl (~23 sccm), and H2 (~4.5 sccm) carrier.
- GaN HEMT Epitaxy: Growth of 1.5 µm GaN, ~2 nm AlN spacer, and 20 nm AlGaN barrier at 1060 °C via MOVPE in an AIX200/4HT-S reactor.
- ELOG Patterning: ICP etching of GaN/AlN/PD template into (10-10) stripes using a ~200 nm Ni mask.
- Mask Fabrication: Deposition of SixNy or SiO2 growth mask, selectively exposing stripe sidewalls for lateral overgrowth.
- Lateral Regrowth: Re-growth on exposed sidewalls to promote lateral (10-10) propagation, bending dislocations 90° and terminating them at lateral surfaces.
- TEM Sample Preparation: Focused ion beam (FIB) lift-out with 2 µm Pt surface protection; rough milling at 30 kV, final polish at 5 kV.
- Electron Microscopy Characterization: Bright-field and two-beam g=(0002) imaging on Philips EM430 (200 kV) and JEOL 2010 (160 kV); CBED polarity determination.
6CCVD Solutions & Capabilities
Section titled “6CCVD Solutions & Capabilities”-
Applicable Materials: For thermal management applications in GaN-on-diamond HEMTs, Optical Grade Polycrystalline Diamond (PCD) wafers are the primary recommendation, offering the high thermal conductivity (~2000 W·m−1·K−1) required for efficient heat extraction from wide-bandgap devices. For research groups seeking to extend toward single-crystal performance, Single Crystal Diamond (SCD) plates from 0.1 µm to 500 µm thickness provide a low-defect-density platform to further reduce GaN nucleation challenges.
-
Substrate Format Compatibility: The 1-2 µm polycrystalline grain size used in this study aligns well with 6CCVD’s standard PCD production. Custom dimensions are available up to 125 mm diameter, with substrate thicknesses up to 10 mm—enabling researchers to scale from coupon-size proof-of-concept to full wafer formats for device fabrication.
-
Surface Engineering for Epitaxy: The low-temperature AlN nucleation strategy used here is sensitive to diamond surface roughness and non-planar defects. 6CCVD’s precision polishing services (Ra <5 nm for inch-size PCD, Ra <1 nm for SCD) directly address the surface quality demands of heteroepitaxial GaN growth, minimizing nucleation pit density and improving buffer layer uniformity.
-
Customization Potential: For ELOG processing workflows requiring patterned GaN/diamond templates, 6CCVD provides laser cutting and dicing services with custom edge geometries. Additionally, in-house metallization capabilities (Ti, W, Au, Pt, Pd, Cu) support the fabrication of back-side thermal contacts and bond layers required for diamond heat-spreader integration in HEMT packages.
-
Engineering Support: 6CCVD’s in-house PhD team can assist with material selection for GaN-on-diamond and other wide-bandgap heterostructure projects—whether optimizing PCD grain morphology for low defect density, selecting appropriate surface termination (H-, O-, or as-grown), or matching CTE profiles for crack mitigation strategies analogous to those demonstrated in this work.
-
Call to Action: For custom specifications, material consultation, or quotes on PCD/SCD substrates tailored to wide-bandgap device research, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract
Transmission and scanning electron microscopy were used to examine the growth of gallium nitride (GaN) on polycrystalline diamond substrates grown by metalorganic vapour phase epitaxy with a low-temperature aluminium nitride (AlN) nucleation layer. Growth on unmasked substrates was in the (0001) orientation with threading dislocation densities ≈7 × 10 9 cm −2 . An epitaxial layer overgrowth technique was used to reduce the dislocation densities further, by depositing silicon nitride stripes on the surface and etching the unmasked regions down to the diamond substrate. A re-growth was then performed on the exposed side walls of the original GaN growth, reducing the threading dislocation density in the overgrown regions by two orders of magnitude. The resulting microstructures and the mechanisms of dislocation reduction are discussed.