Aspheric Cutting of CVD-SiC Molds by PCD milling tool

MetadataDetails
Publication Date2022-01-01
JournalAsian Society for Precision Engineering and Nanotechnology (ASPEN 2022)
AuthorsMirai Sakaida, Tatsuya Furuki, Hirofumi Suzuki, Tatsuya Fukuda
InstitutionsChubu University
AnalysisFull AI Review Included
  • Tool Development: Fabrication of a custom polycrystalline diamond (PCD) milling tool via wire EDM and grinding processes specifically engineered for aspheric ceramic mold machining.
  • Performance Benchmarking: The newly developed PCD tool demonstrated cutting forces equivalent to a conventional #1200 diamond wheel, but delivered superior surface finishes.
  • Surface Finish Achievement (CVD-SiC Mold):
    • Surface roughness: 4 - 6 nm Rz
    • Surface roughness: 0.65 - 0.8 nm Ra
  • Form Accuracy: Achieved an exceptional 0.25 µm P-V (Peak-to-Valley) form accuracy on the aspheric mold after compensation machining.
  • Machining Mode: Validated ductile-mode cutting capability for hard, brittle ceramic materials (CVD-SiC) using the PCD tool.
  • Process Optimization: Implemented compensation machining to counteract tool edge radius errors and tool position errors, reducing form error from 1.1 µm P-V to 0.25 µm P-V.
ParameterValueUnitContext
Tool MaterialPolycrystalline Diamond (PCD)N/ACustom fabricated end mill
Workpiece MaterialCVD-SiC (Silicon Carbide)N/AAspheric ceramic mold
Surface Roughness (Ra)0.65 - 0.8nmAchieved on molded CVD-SiC surface
Surface Roughness (Rz)4 - 6nmAchieved on molded CVD-SiC surface
Initial Form Accuracy1.1µm P-VAfter primary cutting (before compensation)
Final Form Accuracy0.25µm P-VAfter compensation machining
Equivalency Benchmark#1200GritCutting force equivalent to standard diamond wheel
Measurement ToolBlue laser non-contact probeN/AShort wavelength laser scanner
Machining ModeDuctileN/AMode utilized for ceramic mold finishing
Fabrication MethodsWire EDM, GrindingN/ATool shaping processes
  • Tool Fabrication: Manufactured a custom PCD milling tool utilizing wire EDM for initial shaping, followed by grinding for edge preparation.
  • Fundamental Cutting Testing: Conducted baseline cutting force and surface roughness evaluations comparing the PCD tool against conventional diamond wheels.
  • Flat Cutting Experiments: Evaluated surface roughness performance in flat machining scenarios, confirming PCD superiority.
  • Aspherical Machining: Executed precision cutting tests on CVD-SiC aspheric molds.
  • Ductile-Mode Cutting: Engaged ductile material removal mode to machine the brittle ceramic without fracturing the surface.
  • Metrology: Used a non-contact blue laser probe scanner to capture surface profiles, processed via aspheric analysis software.
  • Compensation Algorithm: Analyzed tool edge radius error and tool position error, then applied compensation machining routines to achieve final form accuracy.
  • Applicable Materials: This research relies on high-purity, structurally uniform Polycrystalline Diamond. To replicate or extend these ultra-precision machining results, our Optical Grade PCD or Nano-polycrystalline Diamond plates are ideally suited. For projects requiring extreme edge sharpness and wear resistance, our PCD provides the necessary bulk integrity for wire EDM shaping and grinding.
  • Customization Potential: The study demonstrates the necessity of application-specific tool geometries. 6CCVD provides custom PCD blanks manufactured to your exact dimensional requirements (up to 125mm diameter and thicknesses up to 500µm). Following shaping, our in-house custom metalization (Ti, Pt, Au, etc.) and laser cutting services can tailor the material for final tool assembly.
  • Engineering Support: Achieving 0.65 nm Ra surface finishes demands exceptional substrate homogeneity. 6CCVD’s in-house PhD engineering team can assist with material selection, advising on grain size, purity, and thickness optimizations specific to your ultra-precision machining or mold fabrication requirements.
  • Manufacturing Scalability: Whether you are developing a single bespoke milling tool or scaling up mold production lines, our global manufacturing capabilities ensure supply chain reliability.

For custom specifications, material consultation, or to discuss your precision tooling project requirements, visit 6ccvd.com or contact our engineering team directly.

View Original Abstract

Demands of large molded components with many types of structured surface are increasing in optical device and medical device.Furthermore, structured molds of harder ceramics are required to decrease the mold wear and increase a number of molding times.In order to machine large structured molds of CVD-SiC, large milling tools made of polycrystalline diamond (PCD) were developed.Three hundred cutting edges were generated sharply and precisely by wire EDM and grinding on the edge of a PCD wafer.In the fundamental cutting tests of three types of CVD-SiC with different grain sizes, micro grooves were machined by the developed PCD milling tool, and aspheric cutting tests were carried out.From the experimental results, it was clarified that the developed PCD milling tool was useful for high-efficiency and ultra-precision cutting of CVD-SiC.