On‐Demand, Direct Printing of Nanodiamonds at the Quantum Level (Adv. Sci. 5/2022)
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2022-02-01 |
| Journal | Advanced Science |
| Authors | Zhaoyi Xu, Lingzhi Wang, Huan Xiao, Heekwon Lee, Jihyuk Yang |
| Citations | 1 |
Abstract
Section titled “Abstract”Nanodiamonds Diamond nanocrystals, namely nanodiamonds, hosting point defects such as nitrogen‐vacancy (NV) centers have been emerging as one of the most promising quantum materials. In article number 2103598, Ji Tae Kim, Zhiqin Chu, and co‐workers develop a direct printing method for nanodiamonds containing NV centers at the quantum level. The method developed here provides a high‐precision, lithography‐free route to place diamond defects directly on the universal substrate towards their further developments in many exciting quantum research areas and beyond. [Image: see text]