Probing geometry-induced magnetic defects in cylindrical modulated nanowires with optically detected spin resonance in nitrogen-vacancy center in diamond
At a Glance
Section titled âAt a Glanceâ| Metadata | Details |
|---|---|
| Publication Date | 2024-01-01 |
| Journal | Nanoscale |
| Authors | Umberto Celano, Peter Rickhaus, Cristina Bran, Jorge Marqués-Marchån, Vicent J. Borràs |
| Institutions | National Institute of Materials Physics, Instituto de Ciencia de Materiales de Madrid |
| Citations | 1 |
Abstract
Section titled âAbstractâWe report on magnetic imaging capability with non-perturbative field distribution mapping and minimally invasive magnetic sensing using scanning nitrogen-vacancy magnetometry in axial magnetized nanowires.
Tech Support
Section titled âTech SupportâOriginal Source
Section titled âOriginal SourceâReferences
Section titled âReferencesâ- 2015 - Magnetic Nano- and Microwires [Crossref]