Quantum Control and Waveguide Integration of Diamond Tin-Vacancy Spin Qubits
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2024-01-01 |
| Journal | Quantum 2.0 Conference and Exhibition |
| Authors | Hans K. C. Beukers, Christopher Waas, M. Pasini, Nina Codreanu, Julia M. Brevoord |
| Citations | 1 |
Abstract
Section titled āAbstractāWe show coupling of an SnV center to a diamond waveguide of 20% with almost transform-limited optical transitions. Besides, we show control over the SnV spin qubit and extend its coherence to over a millisecond.